Process for preparing inorganic electroluminescent material

A process for preparing the inorganic electroluminescent material includes such steps as mixing CuI2 and/or CuBr2 and B2O3 and/or Al2O3 with zinc sulfate, covering it by a carbon powder layer, calcining at 1050-1300 deg.C for 2-5 hr, fast cooling acid washing, water washing, mixing it with CuI2 and/...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
1. Verfasser: GUANGZONG,WU QIN
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:A process for preparing the inorganic electroluminescent material includes such steps as mixing CuI2 and/or CuBr2 and B2O3 and/or Al2O3 with zinc sulfate, covering it by a carbon powder layer, calcining at 1050-1300 deg.C for 2-5 hr, fast cooling acid washing, water washing, mixing it with CuI2 and/or CuBr2 and ZnSO4, covering it by a carbon powder layer, calcining at 650-850 deg.C for 2 hr, slow cooling, washing and baking.