Heat-resisant elastic fiber polyurethane modified by diamine montmorillonite and preparation method
The present invention provides a method which uses organic diamine modified montmorillonite as diamine chain-extending agent of polyurethane polymer to make organic diamine montmorillonite/polyurethane nano composite polymer so as to raise heat resistance of polyurethane elastic fibre and raise its...
Gespeichert in:
Hauptverfasser: | , , , , , , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | The present invention provides a method which uses organic diamine modified montmorillonite as diamine chain-extending agent of polyurethane polymer to make organic diamine montmorillonite/polyurethane nano composite polymer so as to raise heat resistance of polyurethane elastic fibre and raise its mechanical property. The described montmorillonite is sodium base montmorillonite, and the polyurethane polymer is formed from polyether polybasic alcohol, isocyanate, linear fatty amine and organic diamine montmorillonite. |
---|