True silk weight raising method
The silk weighting process is to treat the silk to be weighted into weighting agent inside weighting bath. The weighting agent includes emulsifier 3-15 wt%, diglycolic-methacrylic diester 40-80 wt%, sulfate 3-25 wt%, acid 3-15 wt% and detergent 3-15 wt%. The said process can increase the weight of s...
Gespeichert in:
Hauptverfasser: | , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | The silk weighting process is to treat the silk to be weighted into weighting agent inside weighting bath. The weighting agent includes emulsifier 3-15 wt%, diglycolic-methacrylic diester 40-80 wt%, sulfate 3-25 wt%, acid 3-15 wt% and detergent 3-15 wt%. The said process can increase the weight of silk, increase the firm handle, and raise the wool imitating property and wash resistance while maintaining the handle, dyeability and hydroscopic property of silk. The weighting agent is environment friendly. |
---|