Combination of heat conducting materials softend at low temperature, preparation method and application
A heat-conducting composite rubber able to be softened at 38-65 deg.C is prepared through proportionally mixing liquid-state acrylonitrile rubber with vinyl polyacetate, and adding heat-conducting agent chosen from alumina, zinc oxide, aluminium nitride, etc. It can be made into film or heat-conduct...
Gespeichert in:
Hauptverfasser: | , |
---|---|
Format: | Patent |
Sprache: | chi ; eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | A heat-conducting composite rubber able to be softened at 38-65 deg.C is prepared through proportionally mixing liquid-state acrylonitrile rubber with vinyl polyacetate, and adding heat-conducting agent chosen from alumina, zinc oxide, aluminium nitride, etc. It can be made into film or heat-conducting sheet, or for filling it in seam of electronic package or heat radiator.
本发明涉及一种低温软化导热胶材组合物及其制备方法和应用,用分子量300~100000的液态丙烯腈橡胶与聚醋酸乙烯混合,制成软化温度38~65℃的胶材,添加适量的导热剂,如氧化铝、氧化锌、氮化铝,氮化硼、石墨、金属粉或纳米粘土等制成次微米或纳米粉末导热剂,可制成薄膜厚度在0.01~5mm之间,热传导系数在0.5~5W/m-K之间,热阻抗值在0.005~0.2℃m#+[2]/W之间的导热片,且其软化温度范围在38~65℃,可避免存放及运送中液化,用于电子组件与散热器填缝热传导接口,以提高热传导效率。 |
---|