Process for preparing nano-class reinforced rubber or plastic material

A nano-class reinforcing material for rubber or plastics is prepared from calcium lime through hydrous reaction at 20-25 deg.C, stirring while adding dispersion inhibitor, reaction for 30 min, carbnizing reaction at 18-25 deg.C while introducing the mixture of CO2 and air, stirring at 85+/-5 deg.C w...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: JICHUN SU, DESHENG XUE, BAOWEN SU
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:A nano-class reinforcing material for rubber or plastics is prepared from calcium lime through hydrous reaction at 20-25 deg.C, stirring while adding dispersion inhibitor, reaction for 30 min, carbnizing reaction at 18-25 deg.C while introducing the mixture of CO2 and air, stirring at 85+/-5 deg.C while dripping surfactant, activating reaction, ageing for 1 hr, dewatering, drying, and sieving to obtain white powder. Its advantages include high specific surface area, high activated rate and high physical properties.