Splint inlaying technology

Round log is soaked in water at normal temperature, steamed for 6-12 hr, and cut at the timber surface temperature of 70-80 deg.c into splints, the splints are ironed, produced into inlaid figure, painted with hydrochloric acid in the back side, glued, pasted onto board; and the inlaid board is hot...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: XIMING CHEN, JIPU HAN, CONGREN DONG
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Round log is soaked in water at normal temperature, steamed for 6-12 hr, and cut at the timber surface temperature of 70-80 deg.c into splints, the splints are ironed, produced into inlaid figure, painted with hydrochloric acid in the back side, glued, pasted onto board; and the inlaid board is hot pressed, cut and ground. The said technology features no wrapage in the inlaid margin, unified inlaid plane and board plane, high decorative and artistic value, simplified splint inlaying process and perfect inlaying effect.