Process for preparing polymer blends having broad molecular weight distribution in single reactor
Ethylene-based polymer blends having an MWD of at least about 2 are made in a single reactor using a mixed constrained geometry catalyst (CGC) system. The process comprises the steps of contacting under polymerization conditions and in a single reaction vessel (i) ethylene, (ii) at least one C3-C20...
Gespeichert in:
Hauptverfasser: | , , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | Ethylene-based polymer blends having an MWD of at least about 2 are made in a single reactor using a mixed constrained geometry catalyst (CGC) system. The process comprises the steps of contacting under polymerization conditions and in a single reaction vessel (i) ethylene, (ii) at least one C3-C20 alpha-olefin, (iii) optionally, at least one polyene, and (iv) a mixed CGC system. |
---|