Method for stripping two-dimensional nano talc by using organic solvent hydrothermal/expanded two-dimensional nano talc

The invention relates to a method for peeling two-dimensional nano talc by using organic solvent hydrothermal/puffing, which comprises the following steps: S1, crushing: grinding talcum powder to the required particle size, such as 200-5000 meshes; s2, a hydrothermal method: weighing an organic solv...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: WANG PING, LIU WEI, LEE WOO-GUN, WANG ZIYI, WU SUWEN, LIAO SIMIN, ZHU CHUANGGUO, WU YING
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The invention relates to a method for peeling two-dimensional nano talc by using organic solvent hydrothermal/puffing, which comprises the following steps: S1, crushing: grinding talcum powder to the required particle size, such as 200-5000 meshes; s2, a hydrothermal method: weighing an organic solvent with the concentration of 30-100% and talc according to the weight ratio of 1: (0.5-1.5), sequentially pumping the organic solvent and talc into an acid reaction kettle, heating to a boiling point or above, and keeping for 1-72 hours; the invention relates to the technical field of inorganic nonmetallic mineral materials. The prepared two-dimensional nano talcum powder can be effectively applied to the field of inorganic material filling, the filling amount is large, and the strength and toughness of the material are improved. 本发明涉及一种利用有机溶剂水热/膨化二维纳米滑石剥片法,一种利用有机溶剂水热/膨化二维纳米滑石剥片法,包括以下步骤:S1粉碎,将滑石粉磨至所需粒度,如200目-5000目;S2水热法,将有机溶剂按浓度30%-100%与滑石1:0.5-1.5重量比称量,先后泵入酸式反应釜,加热至沸点以上,并保持1h-72h。本发明涉及无机非金属矿物材料的技术领域。本发明制备得到的二维纳米滑