Control method for continuous casting secondary cooling of high-carbon steel slab

The invention provides a high-carbon steel slab continuous casting secondary cooling control method, which comprises the following steps that a secondary cooling area is divided into a first area to a fifth area along a throwing direction, and the cooling strength ratios are 4.3-5.8, 4.1-5.3, 3.6-4....

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: DAI ZHICAI, NIE CHANGPING, LIU HAO, LUO GANG, PENG XIALIN, DENG ZHIXUN, ZHANG PENG, XU GANGJUN, HOU ZEWANG, JIN RENCHUN, XIE SHIZHENG, LIANG LIANG, SONG GANG, XIAO LEI, SUI YAFEI
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator DAI ZHICAI
NIE CHANGPING
LIU HAO
LUO GANG
PENG XIALIN
DENG ZHIXUN
ZHANG PENG
XU GANGJUN
HOU ZEWANG
JIN RENCHUN
XIE SHIZHENG
LIANG LIANG
SONG GANG
XIAO LEI
SUI YAFEI
description The invention provides a high-carbon steel slab continuous casting secondary cooling control method, which comprises the following steps that a secondary cooling area is divided into a first area to a fifth area along a throwing direction, and the cooling strength ratios are 4.3-5.8, 4.1-5.3, 3.6-4.7, 2.0-2.6 and 1.0; in the transverse width of the secondary cooling area, water is distributed to the center part, the secondary middle part and the edge part in sequence according to T center + (-1.3%-2.0%), T secondary middle + (-2.0%-3.2%) and T edge part + (-2.5%-0); wherein the first area, the second area, the third area, the fourth area and the fifth area are sequentially distributed in the secondary cooling area and completely cover the secondary cooling area, and the lengths of the first area, the second area, the third area, the fourth area and the fifth area in the throwing direction are 0.45-0.55 m, 1.4-1.55 m, 2.0-2.2 m, 2.4-2.6 m and 2.45-2.65 m respectively. According to the method, the plate blank i
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN118385500A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN118385500A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN118385500A3</originalsourceid><addsrcrecordid>eNrjZAh0zs8rKcrPUchNLcnIT1FIyy9SSAYKZeaV5pcWKyQnFgOZ6QrFqUDBlMSiSqBkfg5IJD9NISMzPUM3ObEoKT9PobgkNTVHoTgnMYmHgTUtMac4lRdKczMourmGOHvophbkx6cWFyQmp-allsQ7-xkaWhhbmJoaGDgaE6MGAARSN-g</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Control method for continuous casting secondary cooling of high-carbon steel slab</title><source>esp@cenet</source><creator>DAI ZHICAI ; NIE CHANGPING ; LIU HAO ; LUO GANG ; PENG XIALIN ; DENG ZHIXUN ; ZHANG PENG ; XU GANGJUN ; HOU ZEWANG ; JIN RENCHUN ; XIE SHIZHENG ; LIANG LIANG ; SONG GANG ; XIAO LEI ; SUI YAFEI</creator><creatorcontrib>DAI ZHICAI ; NIE CHANGPING ; LIU HAO ; LUO GANG ; PENG XIALIN ; DENG ZHIXUN ; ZHANG PENG ; XU GANGJUN ; HOU ZEWANG ; JIN RENCHUN ; XIE SHIZHENG ; LIANG LIANG ; SONG GANG ; XIAO LEI ; SUI YAFEI</creatorcontrib><description>The invention provides a high-carbon steel slab continuous casting secondary cooling control method, which comprises the following steps that a secondary cooling area is divided into a first area to a fifth area along a throwing direction, and the cooling strength ratios are 4.3-5.8, 4.1-5.3, 3.6-4.7, 2.0-2.6 and 1.0; in the transverse width of the secondary cooling area, water is distributed to the center part, the secondary middle part and the edge part in sequence according to T center + (-1.3%-2.0%), T secondary middle + (-2.0%-3.2%) and T edge part + (-2.5%-0); wherein the first area, the second area, the third area, the fourth area and the fifth area are sequentially distributed in the secondary cooling area and completely cover the secondary cooling area, and the lengths of the first area, the second area, the third area, the fourth area and the fifth area in the throwing direction are 0.45-0.55 m, 1.4-1.55 m, 2.0-2.2 m, 2.4-2.6 m and 2.45-2.65 m respectively. According to the method, the plate blank i</description><language>chi ; eng</language><subject>ALLOYS ; CASTING ; CASTING OF METALS ; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES ; CHEMISTRY ; FERROUS OR NON-FERROUS ALLOYS ; METALLURGY ; PERFORMING OPERATIONS ; POWDER METALLURGY ; TRANSPORTING ; TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><creationdate>2024</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20240726&amp;DB=EPODOC&amp;CC=CN&amp;NR=118385500A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25563,76318</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20240726&amp;DB=EPODOC&amp;CC=CN&amp;NR=118385500A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>DAI ZHICAI</creatorcontrib><creatorcontrib>NIE CHANGPING</creatorcontrib><creatorcontrib>LIU HAO</creatorcontrib><creatorcontrib>LUO GANG</creatorcontrib><creatorcontrib>PENG XIALIN</creatorcontrib><creatorcontrib>DENG ZHIXUN</creatorcontrib><creatorcontrib>ZHANG PENG</creatorcontrib><creatorcontrib>XU GANGJUN</creatorcontrib><creatorcontrib>HOU ZEWANG</creatorcontrib><creatorcontrib>JIN RENCHUN</creatorcontrib><creatorcontrib>XIE SHIZHENG</creatorcontrib><creatorcontrib>LIANG LIANG</creatorcontrib><creatorcontrib>SONG GANG</creatorcontrib><creatorcontrib>XIAO LEI</creatorcontrib><creatorcontrib>SUI YAFEI</creatorcontrib><title>Control method for continuous casting secondary cooling of high-carbon steel slab</title><description>The invention provides a high-carbon steel slab continuous casting secondary cooling control method, which comprises the following steps that a secondary cooling area is divided into a first area to a fifth area along a throwing direction, and the cooling strength ratios are 4.3-5.8, 4.1-5.3, 3.6-4.7, 2.0-2.6 and 1.0; in the transverse width of the secondary cooling area, water is distributed to the center part, the secondary middle part and the edge part in sequence according to T center + (-1.3%-2.0%), T secondary middle + (-2.0%-3.2%) and T edge part + (-2.5%-0); wherein the first area, the second area, the third area, the fourth area and the fifth area are sequentially distributed in the secondary cooling area and completely cover the secondary cooling area, and the lengths of the first area, the second area, the third area, the fourth area and the fifth area in the throwing direction are 0.45-0.55 m, 1.4-1.55 m, 2.0-2.2 m, 2.4-2.6 m and 2.45-2.65 m respectively. According to the method, the plate blank i</description><subject>ALLOYS</subject><subject>CASTING</subject><subject>CASTING OF METALS</subject><subject>CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES</subject><subject>CHEMISTRY</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>METALLURGY</subject><subject>PERFORMING OPERATIONS</subject><subject>POWDER METALLURGY</subject><subject>TRANSPORTING</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2024</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZAh0zs8rKcrPUchNLcnIT1FIyy9SSAYKZeaV5pcWKyQnFgOZ6QrFqUDBlMSiSqBkfg5IJD9NISMzPUM3ObEoKT9PobgkNTVHoTgnMYmHgTUtMac4lRdKczMourmGOHvophbkx6cWFyQmp-allsQ7-xkaWhhbmJoaGDgaE6MGAARSN-g</recordid><startdate>20240726</startdate><enddate>20240726</enddate><creator>DAI ZHICAI</creator><creator>NIE CHANGPING</creator><creator>LIU HAO</creator><creator>LUO GANG</creator><creator>PENG XIALIN</creator><creator>DENG ZHIXUN</creator><creator>ZHANG PENG</creator><creator>XU GANGJUN</creator><creator>HOU ZEWANG</creator><creator>JIN RENCHUN</creator><creator>XIE SHIZHENG</creator><creator>LIANG LIANG</creator><creator>SONG GANG</creator><creator>XIAO LEI</creator><creator>SUI YAFEI</creator><scope>EVB</scope></search><sort><creationdate>20240726</creationdate><title>Control method for continuous casting secondary cooling of high-carbon steel slab</title><author>DAI ZHICAI ; NIE CHANGPING ; LIU HAO ; LUO GANG ; PENG XIALIN ; DENG ZHIXUN ; ZHANG PENG ; XU GANGJUN ; HOU ZEWANG ; JIN RENCHUN ; XIE SHIZHENG ; LIANG LIANG ; SONG GANG ; XIAO LEI ; SUI YAFEI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN118385500A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2024</creationdate><topic>ALLOYS</topic><topic>CASTING</topic><topic>CASTING OF METALS</topic><topic>CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES</topic><topic>CHEMISTRY</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>METALLURGY</topic><topic>PERFORMING OPERATIONS</topic><topic>POWDER METALLURGY</topic><topic>TRANSPORTING</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>DAI ZHICAI</creatorcontrib><creatorcontrib>NIE CHANGPING</creatorcontrib><creatorcontrib>LIU HAO</creatorcontrib><creatorcontrib>LUO GANG</creatorcontrib><creatorcontrib>PENG XIALIN</creatorcontrib><creatorcontrib>DENG ZHIXUN</creatorcontrib><creatorcontrib>ZHANG PENG</creatorcontrib><creatorcontrib>XU GANGJUN</creatorcontrib><creatorcontrib>HOU ZEWANG</creatorcontrib><creatorcontrib>JIN RENCHUN</creatorcontrib><creatorcontrib>XIE SHIZHENG</creatorcontrib><creatorcontrib>LIANG LIANG</creatorcontrib><creatorcontrib>SONG GANG</creatorcontrib><creatorcontrib>XIAO LEI</creatorcontrib><creatorcontrib>SUI YAFEI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>DAI ZHICAI</au><au>NIE CHANGPING</au><au>LIU HAO</au><au>LUO GANG</au><au>PENG XIALIN</au><au>DENG ZHIXUN</au><au>ZHANG PENG</au><au>XU GANGJUN</au><au>HOU ZEWANG</au><au>JIN RENCHUN</au><au>XIE SHIZHENG</au><au>LIANG LIANG</au><au>SONG GANG</au><au>XIAO LEI</au><au>SUI YAFEI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Control method for continuous casting secondary cooling of high-carbon steel slab</title><date>2024-07-26</date><risdate>2024</risdate><abstract>The invention provides a high-carbon steel slab continuous casting secondary cooling control method, which comprises the following steps that a secondary cooling area is divided into a first area to a fifth area along a throwing direction, and the cooling strength ratios are 4.3-5.8, 4.1-5.3, 3.6-4.7, 2.0-2.6 and 1.0; in the transverse width of the secondary cooling area, water is distributed to the center part, the secondary middle part and the edge part in sequence according to T center + (-1.3%-2.0%), T secondary middle + (-2.0%-3.2%) and T edge part + (-2.5%-0); wherein the first area, the second area, the third area, the fourth area and the fifth area are sequentially distributed in the secondary cooling area and completely cover the secondary cooling area, and the lengths of the first area, the second area, the third area, the fourth area and the fifth area in the throwing direction are 0.45-0.55 m, 1.4-1.55 m, 2.0-2.2 m, 2.4-2.6 m and 2.45-2.65 m respectively. According to the method, the plate blank i</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN118385500A
source esp@cenet
subjects ALLOYS
CASTING
CASTING OF METALS
CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES
CHEMISTRY
FERROUS OR NON-FERROUS ALLOYS
METALLURGY
PERFORMING OPERATIONS
POWDER METALLURGY
TRANSPORTING
TREATMENT OF ALLOYS OR NON-FERROUS METALS
title Control method for continuous casting secondary cooling of high-carbon steel slab
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-12T00%3A20%3A43IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=DAI%20ZHICAI&rft.date=2024-07-26&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN118385500A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true