Preparation method of peroxide vulcanized fluororubber with high fluorine content
The invention provides a preparation method of high-fluorine-content peroxide vulcanized fluororubber, which adopts a perfluorinated organic peroxide initiation system to change the polymerization temperature of fluororubber and improve the relative reactivity rate of high-fluorine-content component...
Gespeichert in:
Hauptverfasser: | , , , |
---|---|
Format: | Patent |
Sprache: | chi ; eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | The invention provides a preparation method of high-fluorine-content peroxide vulcanized fluororubber, which adopts a perfluorinated organic peroxide initiation system to change the polymerization temperature of fluororubber and improve the relative reactivity rate of high-fluorine-content components, so that the fluorine content of the product reaches more than 70%; alkyl bromide is used as a chain transfer agent and a vulcanization point monomer, the low Mooney viscosity can reach 30 ML 121 DEG C 1 + 10 or below, bromine atoms are introduced into the molecular structure of the polymer, the effect of a cross-linking point is achieved in peroxide vulcanization, the vulcanization effect is improved, and the phenomena that the vulcanization effect of a vulcanization system becomes poor and the low Mooney viscosity is too high are avoided.
本发明提供了一种高氟含量过氧化物硫化氟橡胶的制备方法,它采用全氟有机过氧化物引发体系改变氟橡胶聚合温度,提高高含氟组分的相对竞聚率,使产物氟含量达到70%以上;使用烷基溴化物作为链转移剂和硫化点单体,既能使低门尼粘度达到30ML121℃1+10以下,又向聚合物的分子结构中引入了溴原子,在过氧化物硫化中起到交联点的作用,改善硫化效果,避免出现硫化体系 |
---|