Bismuth removal agent for lead smelting, preparation method of bismuth removal agent and bismuth removal method
The invention discloses a bismuth removal agent for lead smelting, a preparation method of the bismuth removal agent and a bismuth removal method. The bismuth removal agent comprises the following components in parts by weight: 60-80 parts of calcium magnesium alloy, 2-4 parts of pseudo-boehmite, 1-...
Gespeichert in:
Hauptverfasser: | , , , , , |
---|---|
Format: | Patent |
Sprache: | chi ; eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | SHI HANFEI YANG HONGBO YANG JIAYI YANG HONGLI YANG YIFAN JI HUINA |
description | The invention discloses a bismuth removal agent for lead smelting, a preparation method of the bismuth removal agent and a bismuth removal method. The bismuth removal agent comprises the following components in parts by weight: 60-80 parts of calcium magnesium alloy, 2-4 parts of pseudo-boehmite, 1-3 parts of sodium carbonate, 1-2 parts of sodium sulfate, 3-5 parts of fluorite powder and 2-3 parts of borax. The mass fraction of calcium in the calcium-magnesium alloy is 15-30%. The blocky bismuth removal agent is obtained by preheating the bismuth removal agent, the bismuth removal agent is immersed in lead liquid by using a cage, the characteristic that pseudo-boehmite is decomposed to generate water molecules and form porous gamma-aluminum oxide under a high-temperature condition is utilized, and other components in the bismuth removal agent are matched, so that a relatively high bismuth removal effect can be achieved; and meanwhile, the slag amount is remarkably reduced, the lead recovery rate is improved, |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN118028615A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN118028615A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN118028615A3</originalsourceid><addsrcrecordid>eNqNi7EOAUEQQLdRCP5h9CSWkGu5EJVKfxl29m6T3ZnN7vD9CjoK1Svee2Mjh1DTQwcolOSJEbAnVvBSIBI6qImiBu4XkAtlLKhBGBLpIA7Ew-3njuy-zPuZmpHHWGn24cTMT8dre15Slo5qxjsxadderG1W62Znt_vNP80LHtZDJQ</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Bismuth removal agent for lead smelting, preparation method of bismuth removal agent and bismuth removal method</title><source>esp@cenet</source><creator>SHI HANFEI ; YANG HONGBO ; YANG JIAYI ; YANG HONGLI ; YANG YIFAN ; JI HUINA</creator><creatorcontrib>SHI HANFEI ; YANG HONGBO ; YANG JIAYI ; YANG HONGLI ; YANG YIFAN ; JI HUINA</creatorcontrib><description>The invention discloses a bismuth removal agent for lead smelting, a preparation method of the bismuth removal agent and a bismuth removal method. The bismuth removal agent comprises the following components in parts by weight: 60-80 parts of calcium magnesium alloy, 2-4 parts of pseudo-boehmite, 1-3 parts of sodium carbonate, 1-2 parts of sodium sulfate, 3-5 parts of fluorite powder and 2-3 parts of borax. The mass fraction of calcium in the calcium-magnesium alloy is 15-30%. The blocky bismuth removal agent is obtained by preheating the bismuth removal agent, the bismuth removal agent is immersed in lead liquid by using a cage, the characteristic that pseudo-boehmite is decomposed to generate water molecules and form porous gamma-aluminum oxide under a high-temperature condition is utilized, and other components in the bismuth removal agent are matched, so that a relatively high bismuth removal effect can be achieved; and meanwhile, the slag amount is remarkably reduced, the lead recovery rate is improved,</description><language>chi ; eng</language><subject>CHEMISTRY ; FERROUS OR NON-FERROUS ALLOYS ; METALLURGY ; PRETREATMENT OF RAW MATERIALS ; PRODUCTION AND REFINING OF METALS ; TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><creationdate>2024</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20240514&DB=EPODOC&CC=CN&NR=118028615A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25562,76317</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20240514&DB=EPODOC&CC=CN&NR=118028615A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>SHI HANFEI</creatorcontrib><creatorcontrib>YANG HONGBO</creatorcontrib><creatorcontrib>YANG JIAYI</creatorcontrib><creatorcontrib>YANG HONGLI</creatorcontrib><creatorcontrib>YANG YIFAN</creatorcontrib><creatorcontrib>JI HUINA</creatorcontrib><title>Bismuth removal agent for lead smelting, preparation method of bismuth removal agent and bismuth removal method</title><description>The invention discloses a bismuth removal agent for lead smelting, a preparation method of the bismuth removal agent and a bismuth removal method. The bismuth removal agent comprises the following components in parts by weight: 60-80 parts of calcium magnesium alloy, 2-4 parts of pseudo-boehmite, 1-3 parts of sodium carbonate, 1-2 parts of sodium sulfate, 3-5 parts of fluorite powder and 2-3 parts of borax. The mass fraction of calcium in the calcium-magnesium alloy is 15-30%. The blocky bismuth removal agent is obtained by preheating the bismuth removal agent, the bismuth removal agent is immersed in lead liquid by using a cage, the characteristic that pseudo-boehmite is decomposed to generate water molecules and form porous gamma-aluminum oxide under a high-temperature condition is utilized, and other components in the bismuth removal agent are matched, so that a relatively high bismuth removal effect can be achieved; and meanwhile, the slag amount is remarkably reduced, the lead recovery rate is improved,</description><subject>CHEMISTRY</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>METALLURGY</subject><subject>PRETREATMENT OF RAW MATERIALS</subject><subject>PRODUCTION AND REFINING OF METALS</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2024</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNi7EOAUEQQLdRCP5h9CSWkGu5EJVKfxl29m6T3ZnN7vD9CjoK1Svee2Mjh1DTQwcolOSJEbAnVvBSIBI6qImiBu4XkAtlLKhBGBLpIA7Ew-3njuy-zPuZmpHHWGn24cTMT8dre15Slo5qxjsxadderG1W62Znt_vNP80LHtZDJQ</recordid><startdate>20240514</startdate><enddate>20240514</enddate><creator>SHI HANFEI</creator><creator>YANG HONGBO</creator><creator>YANG JIAYI</creator><creator>YANG HONGLI</creator><creator>YANG YIFAN</creator><creator>JI HUINA</creator><scope>EVB</scope></search><sort><creationdate>20240514</creationdate><title>Bismuth removal agent for lead smelting, preparation method of bismuth removal agent and bismuth removal method</title><author>SHI HANFEI ; YANG HONGBO ; YANG JIAYI ; YANG HONGLI ; YANG YIFAN ; JI HUINA</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN118028615A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2024</creationdate><topic>CHEMISTRY</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>METALLURGY</topic><topic>PRETREATMENT OF RAW MATERIALS</topic><topic>PRODUCTION AND REFINING OF METALS</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>SHI HANFEI</creatorcontrib><creatorcontrib>YANG HONGBO</creatorcontrib><creatorcontrib>YANG JIAYI</creatorcontrib><creatorcontrib>YANG HONGLI</creatorcontrib><creatorcontrib>YANG YIFAN</creatorcontrib><creatorcontrib>JI HUINA</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>SHI HANFEI</au><au>YANG HONGBO</au><au>YANG JIAYI</au><au>YANG HONGLI</au><au>YANG YIFAN</au><au>JI HUINA</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Bismuth removal agent for lead smelting, preparation method of bismuth removal agent and bismuth removal method</title><date>2024-05-14</date><risdate>2024</risdate><abstract>The invention discloses a bismuth removal agent for lead smelting, a preparation method of the bismuth removal agent and a bismuth removal method. The bismuth removal agent comprises the following components in parts by weight: 60-80 parts of calcium magnesium alloy, 2-4 parts of pseudo-boehmite, 1-3 parts of sodium carbonate, 1-2 parts of sodium sulfate, 3-5 parts of fluorite powder and 2-3 parts of borax. The mass fraction of calcium in the calcium-magnesium alloy is 15-30%. The blocky bismuth removal agent is obtained by preheating the bismuth removal agent, the bismuth removal agent is immersed in lead liquid by using a cage, the characteristic that pseudo-boehmite is decomposed to generate water molecules and form porous gamma-aluminum oxide under a high-temperature condition is utilized, and other components in the bismuth removal agent are matched, so that a relatively high bismuth removal effect can be achieved; and meanwhile, the slag amount is remarkably reduced, the lead recovery rate is improved,</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | chi ; eng |
recordid | cdi_epo_espacenet_CN118028615A |
source | esp@cenet |
subjects | CHEMISTRY FERROUS OR NON-FERROUS ALLOYS METALLURGY PRETREATMENT OF RAW MATERIALS PRODUCTION AND REFINING OF METALS TREATMENT OF ALLOYS OR NON-FERROUS METALS |
title | Bismuth removal agent for lead smelting, preparation method of bismuth removal agent and bismuth removal method |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-13T20%3A24%3A59IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=SHI%20HANFEI&rft.date=2024-05-14&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN118028615A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |