Metal ceramic inert anode material with low metal phase content and preparation method

The invention relates to the technical field of anode materials, in particular to a metal ceramic inert anode material with low metal phase content and a preparation method. The metal ceramic inert anode material comprises the following components in percentage by mass: 3-5% of a metal phase and 95-...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: ISHIKI, HOU GUANGHUI, LI DONGSHENG, BAO SHENGZHONG, SHI MENGHAN, LI JING, WANG HUAIJIANG, CHEN KAIBIN, TENG YUAN, MA JUNYI
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The invention relates to the technical field of anode materials, in particular to a metal ceramic inert anode material with low metal phase content and a preparation method. The metal ceramic inert anode material comprises the following components in percentage by mass: 3-5% of a metal phase and 95-97% of a ceramic phase, wherein the metal elements of the metal phase comprise Cu, Ni and Fe; the ceramic phase is prepared from NiFe2O4. 10NiO, TiN, ZrB2 and an oxide additive; by designing the components of the metal ceramic inert anode material, the problem that the conductivity, the corrosion resistance and the thermal shock resistance of a metal ceramic inert anode are difficult to consider at the same time is solved. 本申请涉及阳极材料技术领域,尤其涉及一种低金属相含量的金属陶瓷惰性阳极材料及制备方法;以质量分数计,所述金属陶瓷惰性阳极材料包括:金属相:3%~5%和陶瓷相:95%~97%;其中,所述金属相的金属元素包括Cu、Ni和Fe;所述陶瓷相包括NiFe2O4·10NiO、TiN、ZrB2和氧化物添加剂;通过设计金属陶瓷惰性阳极材料的组分,解决了金属陶瓷惰性阳极电导率、耐腐蚀性和抗热震性能难以兼顾的难题。