Glass ceramic, tempered glass and preparation method and application thereof

The invention relates to microcrystalline glass, tempered glass and a preparation method and application thereof. The microcrystalline glass comprises a spinel crystal phase with the crystallinity greater than 20%; the microcrystalline glass comprises the following components in percentage by mass:...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: LIANG YIBIN, ZHAO BEIYU, XIAO ZIFAN, MAO JIAYING, QING LIPING, PING WENLIANG, KANG QINGWEI, CHEN QIURONG
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator LIANG YIBIN
ZHAO BEIYU
XIAO ZIFAN
MAO JIAYING
QING LIPING
PING WENLIANG
KANG QINGWEI
CHEN QIURONG
description The invention relates to microcrystalline glass, tempered glass and a preparation method and application thereof. The microcrystalline glass comprises a spinel crystal phase with the crystallinity greater than 20%; the microcrystalline glass comprises the following components in percentage by mass: 35% < = SiO2 < = 55%, 15% < = Al2O3 < = 35%, 0% < = Li2O < 1%, 0% < = MgO < = 10%, 0% < = Na2O < = 15%, 5% < = ZnO < = 15%, 0% < = ZrO2 < = 6%, and 0% < = TiO2 < = 6%. The composition of the microcrystalline glass meets the following conditions in percentage by mass: greater than or equal to 67% of SiO2 and Al2O3, greater than or equal to 3% and less than or equal to 8% of ZrO2 and TiO2, less than or equal to 16% of MgO and ZnO, and less than or equal to 0.11 of Li2O/(MgO and ZnO). 本申请涉及一种微晶玻璃、强化玻璃及其制备方法、应用。微晶玻璃包含有结晶度>20%的尖晶石晶相;按质量百分比计,微晶玻璃的组成包括:35%≤SiO2≤55%、15%≤Al2O3≤35%、0%≤Li2O<1%、0%≤MgO≤10%、0%≤Na2O≤15%、5%≤ZnO≤15%、0%≤ZrO2≤6%、及0%≤TiO2≤6%;所述微晶玻璃的组成的质量百分比满足以下条件:SiO2+Al2O3≥67%,3%≤ZrO2+TiO2≤8%,MgO+ZnO≤16%,Li2O/(MgO+Zn
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN117125897A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN117125897A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN117125897A3</originalsourceid><addsrcrecordid>eNrjZPBxz0ksLlZITi1KzM1M1lEoSc0tSC1KTVFIB4sn5qUoFBSlFiQWJZZk5ucp5KaWZOSngIUTCwpyMpMhwiUZQD35aTwMrGmJOcWpvFCam0HRzTXE2UM3tSA_PrW4IDE5NS-1JN7Zz9DQ3NDI1MLS3NGYGDUAjaE13A</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Glass ceramic, tempered glass and preparation method and application thereof</title><source>esp@cenet</source><creator>LIANG YIBIN ; ZHAO BEIYU ; XIAO ZIFAN ; MAO JIAYING ; QING LIPING ; PING WENLIANG ; KANG QINGWEI ; CHEN QIURONG</creator><creatorcontrib>LIANG YIBIN ; ZHAO BEIYU ; XIAO ZIFAN ; MAO JIAYING ; QING LIPING ; PING WENLIANG ; KANG QINGWEI ; CHEN QIURONG</creatorcontrib><description><![CDATA[The invention relates to microcrystalline glass, tempered glass and a preparation method and application thereof. The microcrystalline glass comprises a spinel crystal phase with the crystallinity greater than 20%; the microcrystalline glass comprises the following components in percentage by mass: 35% < = SiO2 < = 55%, 15% < = Al2O3 < = 35%, 0% < = Li2O < 1%, 0% < = MgO < = 10%, 0% < = Na2O < = 15%, 5% < = ZnO < = 15%, 0% < = ZrO2 < = 6%, and 0% < = TiO2 < = 6%. The composition of the microcrystalline glass meets the following conditions in percentage by mass: greater than or equal to 67% of SiO2 and Al2O3, greater than or equal to 3% and less than or equal to 8% of ZrO2 and TiO2, less than or equal to 16% of MgO and ZnO, and less than or equal to 0.11 of Li2O/(MgO and ZnO). 本申请涉及一种微晶玻璃、强化玻璃及其制备方法、应用。微晶玻璃包含有结晶度>20%的尖晶石晶相;按质量百分比计,微晶玻璃的组成包括:35%≤SiO2≤55%、15%≤Al2O3≤35%、0%≤Li2O<1%、0%≤MgO≤10%、0%≤Na2O≤15%、5%≤ZnO≤15%、0%≤ZrO2≤6%、及0%≤TiO2≤6%;所述微晶玻璃的组成的质量百分比满足以下条件:SiO2+Al2O3≥67%,3%≤ZrO2+TiO2≤8%,MgO+ZnO≤16%,Li2O/(MgO+Zn]]></description><language>chi ; eng</language><subject>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS ; CHEMISTRY ; GLASS ; JOINING GLASS TO GLASS OR OTHER MATERIALS ; MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES ; METALLURGY ; MINERAL OR SLAG WOOL ; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS ; SURFACE TREATMENT OF GLASS</subject><creationdate>2023</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20231128&amp;DB=EPODOC&amp;CC=CN&amp;NR=117125897A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25544,76293</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20231128&amp;DB=EPODOC&amp;CC=CN&amp;NR=117125897A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>LIANG YIBIN</creatorcontrib><creatorcontrib>ZHAO BEIYU</creatorcontrib><creatorcontrib>XIAO ZIFAN</creatorcontrib><creatorcontrib>MAO JIAYING</creatorcontrib><creatorcontrib>QING LIPING</creatorcontrib><creatorcontrib>PING WENLIANG</creatorcontrib><creatorcontrib>KANG QINGWEI</creatorcontrib><creatorcontrib>CHEN QIURONG</creatorcontrib><title>Glass ceramic, tempered glass and preparation method and application thereof</title><description><![CDATA[The invention relates to microcrystalline glass, tempered glass and a preparation method and application thereof. The microcrystalline glass comprises a spinel crystal phase with the crystallinity greater than 20%; the microcrystalline glass comprises the following components in percentage by mass: 35% < = SiO2 < = 55%, 15% < = Al2O3 < = 35%, 0% < = Li2O < 1%, 0% < = MgO < = 10%, 0% < = Na2O < = 15%, 5% < = ZnO < = 15%, 0% < = ZrO2 < = 6%, and 0% < = TiO2 < = 6%. The composition of the microcrystalline glass meets the following conditions in percentage by mass: greater than or equal to 67% of SiO2 and Al2O3, greater than or equal to 3% and less than or equal to 8% of ZrO2 and TiO2, less than or equal to 16% of MgO and ZnO, and less than or equal to 0.11 of Li2O/(MgO and ZnO). 本申请涉及一种微晶玻璃、强化玻璃及其制备方法、应用。微晶玻璃包含有结晶度>20%的尖晶石晶相;按质量百分比计,微晶玻璃的组成包括:35%≤SiO2≤55%、15%≤Al2O3≤35%、0%≤Li2O<1%、0%≤MgO≤10%、0%≤Na2O≤15%、5%≤ZnO≤15%、0%≤ZrO2≤6%、及0%≤TiO2≤6%;所述微晶玻璃的组成的质量百分比满足以下条件:SiO2+Al2O3≥67%,3%≤ZrO2+TiO2≤8%,MgO+ZnO≤16%,Li2O/(MgO+Zn]]></description><subject>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS</subject><subject>CHEMISTRY</subject><subject>GLASS</subject><subject>JOINING GLASS TO GLASS OR OTHER MATERIALS</subject><subject>MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES</subject><subject>METALLURGY</subject><subject>MINERAL OR SLAG WOOL</subject><subject>SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS</subject><subject>SURFACE TREATMENT OF GLASS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2023</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZPBxz0ksLlZITi1KzM1M1lEoSc0tSC1KTVFIB4sn5qUoFBSlFiQWJZZk5ucp5KaWZOSngIUTCwpyMpMhwiUZQD35aTwMrGmJOcWpvFCam0HRzTXE2UM3tSA_PrW4IDE5NS-1JN7Zz9DQ3NDI1MLS3NGYGDUAjaE13A</recordid><startdate>20231128</startdate><enddate>20231128</enddate><creator>LIANG YIBIN</creator><creator>ZHAO BEIYU</creator><creator>XIAO ZIFAN</creator><creator>MAO JIAYING</creator><creator>QING LIPING</creator><creator>PING WENLIANG</creator><creator>KANG QINGWEI</creator><creator>CHEN QIURONG</creator><scope>EVB</scope></search><sort><creationdate>20231128</creationdate><title>Glass ceramic, tempered glass and preparation method and application thereof</title><author>LIANG YIBIN ; ZHAO BEIYU ; XIAO ZIFAN ; MAO JIAYING ; QING LIPING ; PING WENLIANG ; KANG QINGWEI ; CHEN QIURONG</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN117125897A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2023</creationdate><topic>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS</topic><topic>CHEMISTRY</topic><topic>GLASS</topic><topic>JOINING GLASS TO GLASS OR OTHER MATERIALS</topic><topic>MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES</topic><topic>METALLURGY</topic><topic>MINERAL OR SLAG WOOL</topic><topic>SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS</topic><topic>SURFACE TREATMENT OF GLASS</topic><toplevel>online_resources</toplevel><creatorcontrib>LIANG YIBIN</creatorcontrib><creatorcontrib>ZHAO BEIYU</creatorcontrib><creatorcontrib>XIAO ZIFAN</creatorcontrib><creatorcontrib>MAO JIAYING</creatorcontrib><creatorcontrib>QING LIPING</creatorcontrib><creatorcontrib>PING WENLIANG</creatorcontrib><creatorcontrib>KANG QINGWEI</creatorcontrib><creatorcontrib>CHEN QIURONG</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>LIANG YIBIN</au><au>ZHAO BEIYU</au><au>XIAO ZIFAN</au><au>MAO JIAYING</au><au>QING LIPING</au><au>PING WENLIANG</au><au>KANG QINGWEI</au><au>CHEN QIURONG</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Glass ceramic, tempered glass and preparation method and application thereof</title><date>2023-11-28</date><risdate>2023</risdate><abstract><![CDATA[The invention relates to microcrystalline glass, tempered glass and a preparation method and application thereof. The microcrystalline glass comprises a spinel crystal phase with the crystallinity greater than 20%; the microcrystalline glass comprises the following components in percentage by mass: 35% < = SiO2 < = 55%, 15% < = Al2O3 < = 35%, 0% < = Li2O < 1%, 0% < = MgO < = 10%, 0% < = Na2O < = 15%, 5% < = ZnO < = 15%, 0% < = ZrO2 < = 6%, and 0% < = TiO2 < = 6%. The composition of the microcrystalline glass meets the following conditions in percentage by mass: greater than or equal to 67% of SiO2 and Al2O3, greater than or equal to 3% and less than or equal to 8% of ZrO2 and TiO2, less than or equal to 16% of MgO and ZnO, and less than or equal to 0.11 of Li2O/(MgO and ZnO). 本申请涉及一种微晶玻璃、强化玻璃及其制备方法、应用。微晶玻璃包含有结晶度>20%的尖晶石晶相;按质量百分比计,微晶玻璃的组成包括:35%≤SiO2≤55%、15%≤Al2O3≤35%、0%≤Li2O<1%、0%≤MgO≤10%、0%≤Na2O≤15%、5%≤ZnO≤15%、0%≤ZrO2≤6%、及0%≤TiO2≤6%;所述微晶玻璃的组成的质量百分比满足以下条件:SiO2+Al2O3≥67%,3%≤ZrO2+TiO2≤8%,MgO+ZnO≤16%,Li2O/(MgO+Zn]]></abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN117125897A
source esp@cenet
subjects CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS
CHEMISTRY
GLASS
JOINING GLASS TO GLASS OR OTHER MATERIALS
MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
METALLURGY
MINERAL OR SLAG WOOL
SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS
SURFACE TREATMENT OF GLASS
title Glass ceramic, tempered glass and preparation method and application thereof
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-27T15%3A50%3A31IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=LIANG%20YIBIN&rft.date=2023-11-28&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN117125897A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true