Manufacturing method of colored glass

The invention discloses a manufacturing method of colored glass. The manufacturing method comprises the following specific steps: depositing a photonic crystal coating liquid on a substrate which does not change at 600 DEG C, depositing a ceramic precursor material after drying, sintering at 400-600...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: JIN XIAOLING, WU WEI, SONG YANLIN, YANG MING, WANG MAOXUAN
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator JIN XIAOLING
WU WEI
SONG YANLIN
YANG MING
WANG MAOXUAN
description The invention discloses a manufacturing method of colored glass. The manufacturing method comprises the following specific steps: depositing a photonic crystal coating liquid on a substrate which does not change at 600 DEG C, depositing a ceramic precursor material after drying, sintering at 400-600 DEG C, coating a sintered product with glass powder or a glass powder dispersion liquid which can be molten at 500 DEG C or below, and heating and melting the glass powder. The color glass prepared by the method has the advantages of light transmittance, high strength and hardness, and photonic forbidden band structure color realized by the inverse opal structure. 本发明公开了彩色玻璃的制作方法。所述制作方法的具体步骤为:在600℃不发生变化的基板上沉积光子晶体涂布液,干燥后沉积陶瓷前驱体材料,400-600℃下烧结,在烧结产物上涂布可在500℃以下熔融的玻璃粉或玻璃粉分散液,加热熔融玻璃粉即得。此方法制备的彩色玻璃具有可透光性、较高的强度和硬度、以及通过反蛋白石结构实现的光子禁带结构色彩。
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN116639885A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN116639885A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN116639885A3</originalsourceid><addsrcrecordid>eNrjZFD1TcwrTUtMLiktysxLV8hNLcnIT1HIT1NIzs_JL0pNUUjPSSwu5mFgTUvMKU7lhdLcDIpuriHOHrqpBfnxqcUFicmpeakl8c5-hoZmZsaWFhamjsbEqAEAS-knVg</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Manufacturing method of colored glass</title><source>esp@cenet</source><creator>JIN XIAOLING ; WU WEI ; SONG YANLIN ; YANG MING ; WANG MAOXUAN</creator><creatorcontrib>JIN XIAOLING ; WU WEI ; SONG YANLIN ; YANG MING ; WANG MAOXUAN</creatorcontrib><description>The invention discloses a manufacturing method of colored glass. The manufacturing method comprises the following specific steps: depositing a photonic crystal coating liquid on a substrate which does not change at 600 DEG C, depositing a ceramic precursor material after drying, sintering at 400-600 DEG C, coating a sintered product with glass powder or a glass powder dispersion liquid which can be molten at 500 DEG C or below, and heating and melting the glass powder. The color glass prepared by the method has the advantages of light transmittance, high strength and hardness, and photonic forbidden band structure color realized by the inverse opal structure. 本发明公开了彩色玻璃的制作方法。所述制作方法的具体步骤为:在600℃不发生变化的基板上沉积光子晶体涂布液,干燥后沉积陶瓷前驱体材料,400-600℃下烧结,在烧结产物上涂布可在500℃以下熔融的玻璃粉或玻璃粉分散液,加热熔融玻璃粉即得。此方法制备的彩色玻璃具有可透光性、较高的强度和硬度、以及通过反蛋白石结构实现的光子禁带结构色彩。</description><language>chi ; eng</language><subject>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS ; CHEMISTRY ; GLASS ; JOINING GLASS TO GLASS OR OTHER MATERIALS ; METALLURGY ; MINERAL OR SLAG WOOL ; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS ; SURFACE TREATMENT OF GLASS</subject><creationdate>2023</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20230825&amp;DB=EPODOC&amp;CC=CN&amp;NR=116639885A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20230825&amp;DB=EPODOC&amp;CC=CN&amp;NR=116639885A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>JIN XIAOLING</creatorcontrib><creatorcontrib>WU WEI</creatorcontrib><creatorcontrib>SONG YANLIN</creatorcontrib><creatorcontrib>YANG MING</creatorcontrib><creatorcontrib>WANG MAOXUAN</creatorcontrib><title>Manufacturing method of colored glass</title><description>The invention discloses a manufacturing method of colored glass. The manufacturing method comprises the following specific steps: depositing a photonic crystal coating liquid on a substrate which does not change at 600 DEG C, depositing a ceramic precursor material after drying, sintering at 400-600 DEG C, coating a sintered product with glass powder or a glass powder dispersion liquid which can be molten at 500 DEG C or below, and heating and melting the glass powder. The color glass prepared by the method has the advantages of light transmittance, high strength and hardness, and photonic forbidden band structure color realized by the inverse opal structure. 本发明公开了彩色玻璃的制作方法。所述制作方法的具体步骤为:在600℃不发生变化的基板上沉积光子晶体涂布液,干燥后沉积陶瓷前驱体材料,400-600℃下烧结,在烧结产物上涂布可在500℃以下熔融的玻璃粉或玻璃粉分散液,加热熔融玻璃粉即得。此方法制备的彩色玻璃具有可透光性、较高的强度和硬度、以及通过反蛋白石结构实现的光子禁带结构色彩。</description><subject>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS</subject><subject>CHEMISTRY</subject><subject>GLASS</subject><subject>JOINING GLASS TO GLASS OR OTHER MATERIALS</subject><subject>METALLURGY</subject><subject>MINERAL OR SLAG WOOL</subject><subject>SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS</subject><subject>SURFACE TREATMENT OF GLASS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2023</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZFD1TcwrTUtMLiktysxLV8hNLcnIT1HIT1NIzs_JL0pNUUjPSSwu5mFgTUvMKU7lhdLcDIpuriHOHrqpBfnxqcUFicmpeakl8c5-hoZmZsaWFhamjsbEqAEAS-knVg</recordid><startdate>20230825</startdate><enddate>20230825</enddate><creator>JIN XIAOLING</creator><creator>WU WEI</creator><creator>SONG YANLIN</creator><creator>YANG MING</creator><creator>WANG MAOXUAN</creator><scope>EVB</scope></search><sort><creationdate>20230825</creationdate><title>Manufacturing method of colored glass</title><author>JIN XIAOLING ; WU WEI ; SONG YANLIN ; YANG MING ; WANG MAOXUAN</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN116639885A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2023</creationdate><topic>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS</topic><topic>CHEMISTRY</topic><topic>GLASS</topic><topic>JOINING GLASS TO GLASS OR OTHER MATERIALS</topic><topic>METALLURGY</topic><topic>MINERAL OR SLAG WOOL</topic><topic>SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS</topic><topic>SURFACE TREATMENT OF GLASS</topic><toplevel>online_resources</toplevel><creatorcontrib>JIN XIAOLING</creatorcontrib><creatorcontrib>WU WEI</creatorcontrib><creatorcontrib>SONG YANLIN</creatorcontrib><creatorcontrib>YANG MING</creatorcontrib><creatorcontrib>WANG MAOXUAN</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>JIN XIAOLING</au><au>WU WEI</au><au>SONG YANLIN</au><au>YANG MING</au><au>WANG MAOXUAN</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Manufacturing method of colored glass</title><date>2023-08-25</date><risdate>2023</risdate><abstract>The invention discloses a manufacturing method of colored glass. The manufacturing method comprises the following specific steps: depositing a photonic crystal coating liquid on a substrate which does not change at 600 DEG C, depositing a ceramic precursor material after drying, sintering at 400-600 DEG C, coating a sintered product with glass powder or a glass powder dispersion liquid which can be molten at 500 DEG C or below, and heating and melting the glass powder. The color glass prepared by the method has the advantages of light transmittance, high strength and hardness, and photonic forbidden band structure color realized by the inverse opal structure. 本发明公开了彩色玻璃的制作方法。所述制作方法的具体步骤为:在600℃不发生变化的基板上沉积光子晶体涂布液,干燥后沉积陶瓷前驱体材料,400-600℃下烧结,在烧结产物上涂布可在500℃以下熔融的玻璃粉或玻璃粉分散液,加热熔融玻璃粉即得。此方法制备的彩色玻璃具有可透光性、较高的强度和硬度、以及通过反蛋白石结构实现的光子禁带结构色彩。</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN116639885A
source esp@cenet
subjects CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS
CHEMISTRY
GLASS
JOINING GLASS TO GLASS OR OTHER MATERIALS
METALLURGY
MINERAL OR SLAG WOOL
SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS
SURFACE TREATMENT OF GLASS
title Manufacturing method of colored glass
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-27T14%3A23%3A12IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=JIN%20XIAOLING&rft.date=2023-08-25&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN116639885A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true