Method for smelting nickel-containing molten steel in converter and nickel-containing molten steel

The invention discloses a method for smelting nickel-containing molten steel through a converter and the nickel-containing molten steel. The method comprises the steps that nickel-containing alloy or nickel elementary substance is added into molten iron, oxygen is supplied to the molten iron through...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: MA YINGJIAN, TONG ZHIBO, QI JIANGHUA, LIU PENG, XIE CHENG, LI GUOCANG, YAN LIXIN, XIAO AIDA, LUO GANG, TAN DAJIN, YU QIANG, WU PINGHUI, ZHU ZHENLAI, WANG JING, LIU YISI, DENG ZHIXUN, CHEN JIE, LIU HONGJUN, ZHOU JIANFENG, XU GANGJUN, DONG CHANGFU, DENG BIRONG, PENG QICHUN, LIANG LIANG
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The invention discloses a method for smelting nickel-containing molten steel through a converter and the nickel-containing molten steel. The method comprises the steps that nickel-containing alloy or nickel elementary substance is added into molten iron, oxygen is supplied to the molten iron through an oxygen lance, calcium-containing flux is added in batches, the lance position of the oxygen lance is 150-240 cm, the oxygen flow is 700-900 Nm < 3 >/min, and under the condition that oxygen supply is a first oxygen step, the lance position of the oxygen lance is controlled to be 200-240 cm, and the oxygen flow is controlled to be 800-900 Nm < 3 >/min; under the condition that oxygen supply is the second oxygen step, the lance position of the oxygen lance is controlled to be 180-195 cm, and the oxygen flow is 750-870 Nm < 3 >/min; under the condition that oxygen supply is performed in the third oxygen step, the lance position of the oxygen lance is controlled to be 180-195 cm, and the oxygen flow is 730-780 Nm