Method for avoiding rolling failure of 5083 aluminum alloy super-thick cast ingot

The invention relates to aluminum alloy heat treatment, in particular to a method for avoiding rolling failure of a 5083 aluminum alloy super-thick cast ingot, which comprises the following steps of: sequentially carrying out first-section, second-section and third-section homogenizing heat treatmen...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: JIANG XIANQUAN, SHE XINWEI, YU JIANGYANG, DU WEICHANG, TIAN YUHE
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The invention relates to aluminum alloy heat treatment, in particular to a method for avoiding rolling failure of a 5083 aluminum alloy super-thick cast ingot, which comprises the following steps of: sequentially carrying out first-section, second-section and third-section homogenizing heat treatment on the 5083 aluminum alloy super-thick cast ingot, and directly carrying out hot rolling after the homogenizing heat treatment is finished; the heating temperature of the first-section homogenizing heat treatment is 1t; the temperature preset value and the heat preservation time lt; a heat preservation time preset value; the heating temperature of the second-stage homogenization heat treatment is equal to the temperature preset value, and the heat preservation time is 1t; a heat preservation time preset value; the heating temperature of the third-section homogenizing heat treatment is 1t; the heat preservation time is equal to the heat preservation time preset value; the preset temperature value is 470-520 DEG C,