PET modified material as well as preparation method and application thereof
The invention provides a PET modified material as well as a preparation method and application thereof. The PET modified material is prepared from the following components in percentage by mass: 45 to 90 weight percent of polyethylene glycol terephthalate, 0 to 20 weight percent of heat-conducting f...
Gespeichert in:
Hauptverfasser: | , , , , , |
---|---|
Format: | Patent |
Sprache: | chi ; eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | The invention provides a PET modified material as well as a preparation method and application thereof. The PET modified material is prepared from the following components in percentage by mass: 45 to 90 weight percent of polyethylene glycol terephthalate, 0 to 20 weight percent of heat-conducting filler, 1.3 to 6.4 weight percent of additive and 7 to 50 weight percent of glass fiber. Wherein the melt index of the PET modified material is 10 g/10 min to 20 g/10 min. The PET modified material has high molecular weight, and the mechanical property of the PET modified material can be improved.
本申请提供了一种PET改性材料及其制备方法和应用。制备该PET改性材料包括以下质量百分比的组分:聚对苯二甲酸乙二醇酯45wt%~90wt%、导热填料0wt%~20wt%、助剂1.3wt%~6.4wt%、玻璃纤维7wt%~50wt%;其中,PET改性材料的熔融指数为10g/10min~20g/10min。该PET改性材料具有较高的分子量,有利于提升其PET改性材料的力学性能。 |
---|