Aromatization fluidized bed catalyst and preparation method thereof
The invention discloses an aromatization fluidized bed catalyst and a preparation method thereof. The aromatization fluidized bed catalyst comprises the following components: a) 0.5%-20% of at least one selected from first metal element oxides; b) 0.5%-15% of an oxide of at least one selected from P...
Gespeichert in:
Hauptverfasser: | , , |
---|---|
Format: | Patent |
Sprache: | chi ; eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | The invention discloses an aromatization fluidized bed catalyst and a preparation method thereof. The aromatization fluidized bed catalyst comprises the following components: a) 0.5%-20% of at least one selected from first metal element oxides; b) 0.5%-15% of an oxide of at least one selected from P, B, Si, a second metal element, a rare earth element or a noble metal element; c) 30%-60% of a molecular sieve; d) 10%-30% of a component selected from a binder; e) 20%-65% of modified kaolin; wherein the specific surface area of the modified kaolin is 25-100m < 2 >/g. The aromatization fluidized bed catalyst has the advantages of low wear index and high aromatic hydrocarbon yield.
本发明公开了一种芳构化流化床催化剂及其制备方法。本发明芳构化流化床催化剂,包括以下组分:a)0.5%~20%选自第一金属元素氧化物中的至少一种;b)0.5%~15%选自P、B、Si、第二金属元素、稀土元素或贵金属元素中的至少一种的氧化物;c)30%~60%选自分子筛;d)10%~30%选自粘结剂组分;e)20%~65%选自改性高岭土;其中,所述改性高岭土的比表面积为25~100m2/g。该芳构化流化床催化剂具有磨损指数低与芳烃收率高的优点。 |
---|