Emulsified asphalt rubber powder fiber thin slurry mixture penetration type pavement and construction process
The invention relates to an emulsified asphalt rubber powder fiber thin slurry mixture penetration type pavement and a construction process. Every 1000 m < 2 > of the pavement is prepared from the following raw materials by volume: 0.3 m < 3 >-0.6 m < 3 > of asphalt sprayed for the...
Gespeichert in:
Hauptverfasser: | , , , , , , , , , |
---|---|
Format: | Patent |
Sprache: | chi ; eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | The invention relates to an emulsified asphalt rubber powder fiber thin slurry mixture penetration type pavement and a construction process. Every 1000 m < 2 > of the pavement is prepared from the following raw materials by volume: 0.3 m < 3 >-0.6 m < 3 > of asphalt sprayed for the first time, 10 m < 3 >-50 m < 3 > of crushed stone sprayed for the second time, 0.3 m < 3 >-0.6 m < 3 > of asphalt sprayed for the second time, and 10 m < 3 >-40 m < 3 > of an emulsified asphalt rubber powder fiber thin slurry mixture as a penetration material. The construction process comprises the following steps: firstly, sequentially spraying/spreading hot asphalt and broken stones with the particle size of equal thickness, then stabilizing the pressure of the broken stones, then spraying emulsified asphalt, mixing, paving and injecting an emulsified asphalt rubber powder fiber thin slurry mixture, and then carrying out vacuum water absorption and rolling to obtain the emulsified asphalt rubber powder fiber thin slurry mixture |
---|