Alloy powder for SLM, nickel-based alloy with high mechanical property and preparation method of nickel-based alloy

The invention discloses alloy powder for SLM (selective laser melting). The alloy powder comprises the following components in percentage by weight: 19.0%-19.5% of Cr, 17.0%-17.5% of Fe, 3.0%-3.2% of Mo, 0.9%-1% of Ti, 0.52%-0.56% of Al, 5.1%-5.2% of Nb, 0.2%-0.25% of Mn, 0.04%-0.06% of Co, 0.3%-0.3...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: LIU TONG, WANG GANG, DING MAN, ZHU XIEBIN, XUE WANGYANG, LI JIANSHENG, ZHAO YU
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The invention discloses alloy powder for SLM (selective laser melting). The alloy powder comprises the following components in percentage by weight: 19.0%-19.5% of Cr, 17.0%-17.5% of Fe, 3.0%-3.2% of Mo, 0.9%-1% of Ti, 0.52%-0.56% of Al, 5.1%-5.2% of Nb, 0.2%-0.25% of Mn, 0.04%-0.06% of Co, 0.3%-0.35% of Si and the balance of Ni. The invention further discloses a preparation method of the high-mechanical-property nickel-based alloy, and the preparation method comprises the following steps: taking the alloy powder for additive production, spreading the powder, and then performing selective laser melting forming to obtain the high-mechanical-property nickel-based alloy. The invention further discloses the nickel-based alloy with the high mechanical performance. The nickel-based alloy prepared by the invention has few micro-cracks and holes, and has good mechanical properties. 本发明公开了一种SLM用合金粉末,其成分按重量百分比计包括:Cr19.0-19.5%,Fe17.0-17.5%,Mo3.0-3.2%,Ti0.9-1%,Al0.52-0.56%,Nb5.1-5.2%,Mn0.2-0.25%,Co0.04-0.06%,Si0.3-0.35%,