Method for regenerating silicon powder by using waste molding compound as raw material, regenerated silicon powder and epoxy molding compound for TO packaging

The invention belongs to the technical field of resource utilization of waste plastic packaging materials, and particularly relates to a method for regenerating silicon powder by taking waste plastic packaging materials as raw materials, regenerated silicon powder and an epoxy plastic packaging mate...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: LU XUKUI, FENG ZHUOXING, WANG SHANXUE, LI HAILIANG, LI JIANRONG, LI GANG, CHANG ZHIGUO
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator LU XUKUI
FENG ZHUOXING
WANG SHANXUE
LI HAILIANG
LI JIANRONG
LI GANG
CHANG ZHIGUO
description The invention belongs to the technical field of resource utilization of waste plastic packaging materials, and particularly relates to a method for regenerating silicon powder by taking waste plastic packaging materials as raw materials, regenerated silicon powder and an epoxy plastic packaging material for TO packaging. The method comprises the following steps: crushing the waste plastic packaging material, roasting under a stirring condition, and carrying out magnetic separation; carrying out ball milling on the obtained material, and carrying out magnetic separation to obtain regenerated silicon powder; the roasting conditions are as follows: the roasting temperature is 800-1000 DEG C, and the roasting time is 8-15 hours. The obtained regenerated silicon powder can be used for TO-series epoxy molding compounds for packaging, and has important significance for saving the cost of materials used by the molding compounds. 本发明属于废旧塑封料资源化利用技术领域,具体涉及一种以废旧塑封料为原料进行硅粉再生的方法、再生硅粉、TO封装用环氧塑封料。该方法包括以下步骤:将废旧塑封料粉碎,在搅拌条件下进行焙
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN115676843A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN115676843A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN115676843A3</originalsourceid><addsrcrecordid>eNqNjrEKwkAMhrs4iPoOcdehVKurFMVFXbqX2Evr4fVy3F2pfRmf1SsIgi5OIfm_fMk4ep7I31hAxRYs1aTJope6BieVLFmD4U6QhWsPrRvmHTpP0LASQ1dyY7jVAtCBxQ4a9GQlqsVHRuLbhYEnw4_-VzO8kV_AYHnHOiTTaFShcjR710k0P-zz7LgM-wW5wIUjvsjOcbxON-l2leySf5gXwN5U1w</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Method for regenerating silicon powder by using waste molding compound as raw material, regenerated silicon powder and epoxy molding compound for TO packaging</title><source>esp@cenet</source><creator>LU XUKUI ; FENG ZHUOXING ; WANG SHANXUE ; LI HAILIANG ; LI JIANRONG ; LI GANG ; CHANG ZHIGUO</creator><creatorcontrib>LU XUKUI ; FENG ZHUOXING ; WANG SHANXUE ; LI HAILIANG ; LI JIANRONG ; LI GANG ; CHANG ZHIGUO</creatorcontrib><description>The invention belongs to the technical field of resource utilization of waste plastic packaging materials, and particularly relates to a method for regenerating silicon powder by taking waste plastic packaging materials as raw materials, regenerated silicon powder and an epoxy plastic packaging material for TO packaging. The method comprises the following steps: crushing the waste plastic packaging material, roasting under a stirring condition, and carrying out magnetic separation; carrying out ball milling on the obtained material, and carrying out magnetic separation to obtain regenerated silicon powder; the roasting conditions are as follows: the roasting temperature is 800-1000 DEG C, and the roasting time is 8-15 hours. The obtained regenerated silicon powder can be used for TO-series epoxy molding compounds for packaging, and has important significance for saving the cost of materials used by the molding compounds. 本发明属于废旧塑封料资源化利用技术领域,具体涉及一种以废旧塑封料为原料进行硅粉再生的方法、再生硅粉、TO封装用环氧塑封料。该方法包括以下步骤:将废旧塑封料粉碎,在搅拌条件下进行焙</description><language>chi ; eng</language><subject>CHEMISTRY ; COMPOSITIONS BASED THEREON ; COMPOSITIONS OF MACROMOLECULAR COMPOUNDS ; COMPOUNDS THEREOF ; INORGANIC CHEMISTRY ; METALLURGY ; NON-METALLIC ELEMENTS ; ORGANIC MACROMOLECULAR COMPOUNDS ; THEIR PREPARATION OR CHEMICAL WORKING-UP ; USE OF INORGANIC OR NON-MACROMOLECULAR ORGANIC SUBSTANCES ASCOMPOUNDING INGREDIENTS</subject><creationdate>2023</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20230203&amp;DB=EPODOC&amp;CC=CN&amp;NR=115676843A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76289</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20230203&amp;DB=EPODOC&amp;CC=CN&amp;NR=115676843A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>LU XUKUI</creatorcontrib><creatorcontrib>FENG ZHUOXING</creatorcontrib><creatorcontrib>WANG SHANXUE</creatorcontrib><creatorcontrib>LI HAILIANG</creatorcontrib><creatorcontrib>LI JIANRONG</creatorcontrib><creatorcontrib>LI GANG</creatorcontrib><creatorcontrib>CHANG ZHIGUO</creatorcontrib><title>Method for regenerating silicon powder by using waste molding compound as raw material, regenerated silicon powder and epoxy molding compound for TO packaging</title><description>The invention belongs to the technical field of resource utilization of waste plastic packaging materials, and particularly relates to a method for regenerating silicon powder by taking waste plastic packaging materials as raw materials, regenerated silicon powder and an epoxy plastic packaging material for TO packaging. The method comprises the following steps: crushing the waste plastic packaging material, roasting under a stirring condition, and carrying out magnetic separation; carrying out ball milling on the obtained material, and carrying out magnetic separation to obtain regenerated silicon powder; the roasting conditions are as follows: the roasting temperature is 800-1000 DEG C, and the roasting time is 8-15 hours. The obtained regenerated silicon powder can be used for TO-series epoxy molding compounds for packaging, and has important significance for saving the cost of materials used by the molding compounds. 本发明属于废旧塑封料资源化利用技术领域,具体涉及一种以废旧塑封料为原料进行硅粉再生的方法、再生硅粉、TO封装用环氧塑封料。该方法包括以下步骤:将废旧塑封料粉碎,在搅拌条件下进行焙</description><subject>CHEMISTRY</subject><subject>COMPOSITIONS BASED THEREON</subject><subject>COMPOSITIONS OF MACROMOLECULAR COMPOUNDS</subject><subject>COMPOUNDS THEREOF</subject><subject>INORGANIC CHEMISTRY</subject><subject>METALLURGY</subject><subject>NON-METALLIC ELEMENTS</subject><subject>ORGANIC MACROMOLECULAR COMPOUNDS</subject><subject>THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><subject>USE OF INORGANIC OR NON-MACROMOLECULAR ORGANIC SUBSTANCES ASCOMPOUNDING INGREDIENTS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2023</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNjrEKwkAMhrs4iPoOcdehVKurFMVFXbqX2Evr4fVy3F2pfRmf1SsIgi5OIfm_fMk4ep7I31hAxRYs1aTJope6BieVLFmD4U6QhWsPrRvmHTpP0LASQ1dyY7jVAtCBxQ4a9GQlqsVHRuLbhYEnw4_-VzO8kV_AYHnHOiTTaFShcjR710k0P-zz7LgM-wW5wIUjvsjOcbxON-l2leySf5gXwN5U1w</recordid><startdate>20230203</startdate><enddate>20230203</enddate><creator>LU XUKUI</creator><creator>FENG ZHUOXING</creator><creator>WANG SHANXUE</creator><creator>LI HAILIANG</creator><creator>LI JIANRONG</creator><creator>LI GANG</creator><creator>CHANG ZHIGUO</creator><scope>EVB</scope></search><sort><creationdate>20230203</creationdate><title>Method for regenerating silicon powder by using waste molding compound as raw material, regenerated silicon powder and epoxy molding compound for TO packaging</title><author>LU XUKUI ; FENG ZHUOXING ; WANG SHANXUE ; LI HAILIANG ; LI JIANRONG ; LI GANG ; CHANG ZHIGUO</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN115676843A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2023</creationdate><topic>CHEMISTRY</topic><topic>COMPOSITIONS BASED THEREON</topic><topic>COMPOSITIONS OF MACROMOLECULAR COMPOUNDS</topic><topic>COMPOUNDS THEREOF</topic><topic>INORGANIC CHEMISTRY</topic><topic>METALLURGY</topic><topic>NON-METALLIC ELEMENTS</topic><topic>ORGANIC MACROMOLECULAR COMPOUNDS</topic><topic>THEIR PREPARATION OR CHEMICAL WORKING-UP</topic><topic>USE OF INORGANIC OR NON-MACROMOLECULAR ORGANIC SUBSTANCES ASCOMPOUNDING INGREDIENTS</topic><toplevel>online_resources</toplevel><creatorcontrib>LU XUKUI</creatorcontrib><creatorcontrib>FENG ZHUOXING</creatorcontrib><creatorcontrib>WANG SHANXUE</creatorcontrib><creatorcontrib>LI HAILIANG</creatorcontrib><creatorcontrib>LI JIANRONG</creatorcontrib><creatorcontrib>LI GANG</creatorcontrib><creatorcontrib>CHANG ZHIGUO</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>LU XUKUI</au><au>FENG ZHUOXING</au><au>WANG SHANXUE</au><au>LI HAILIANG</au><au>LI JIANRONG</au><au>LI GANG</au><au>CHANG ZHIGUO</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Method for regenerating silicon powder by using waste molding compound as raw material, regenerated silicon powder and epoxy molding compound for TO packaging</title><date>2023-02-03</date><risdate>2023</risdate><abstract>The invention belongs to the technical field of resource utilization of waste plastic packaging materials, and particularly relates to a method for regenerating silicon powder by taking waste plastic packaging materials as raw materials, regenerated silicon powder and an epoxy plastic packaging material for TO packaging. The method comprises the following steps: crushing the waste plastic packaging material, roasting under a stirring condition, and carrying out magnetic separation; carrying out ball milling on the obtained material, and carrying out magnetic separation to obtain regenerated silicon powder; the roasting conditions are as follows: the roasting temperature is 800-1000 DEG C, and the roasting time is 8-15 hours. The obtained regenerated silicon powder can be used for TO-series epoxy molding compounds for packaging, and has important significance for saving the cost of materials used by the molding compounds. 本发明属于废旧塑封料资源化利用技术领域,具体涉及一种以废旧塑封料为原料进行硅粉再生的方法、再生硅粉、TO封装用环氧塑封料。该方法包括以下步骤:将废旧塑封料粉碎,在搅拌条件下进行焙</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN115676843A
source esp@cenet
subjects CHEMISTRY
COMPOSITIONS BASED THEREON
COMPOSITIONS OF MACROMOLECULAR COMPOUNDS
COMPOUNDS THEREOF
INORGANIC CHEMISTRY
METALLURGY
NON-METALLIC ELEMENTS
ORGANIC MACROMOLECULAR COMPOUNDS
THEIR PREPARATION OR CHEMICAL WORKING-UP
USE OF INORGANIC OR NON-MACROMOLECULAR ORGANIC SUBSTANCES ASCOMPOUNDING INGREDIENTS
title Method for regenerating silicon powder by using waste molding compound as raw material, regenerated silicon powder and epoxy molding compound for TO packaging
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-11T18%3A02%3A04IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=LU%20XUKUI&rft.date=2023-02-03&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN115676843A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true