Preparation method of MoO2 and Mn2P2O7 mixed material
The invention provides a preparation method of a MoO2 and Mn2P2O7 mixed material. The preparation method comprises the following steps: S1, putting a molybdenum source and a manganese source into ionic liquid, and heating at a set temperature for a certain time to synthesize a precursor; and S2, mix...
Gespeichert in:
Hauptverfasser: | , |
---|---|
Format: | Patent |
Sprache: | chi ; eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | The invention provides a preparation method of a MoO2 and Mn2P2O7 mixed material. The preparation method comprises the following steps: S1, putting a molybdenum source and a manganese source into ionic liquid, and heating at a set temperature for a certain time to synthesize a precursor; and S2, mixing the precursor with sodium hydrogen hypophosphite, and calcining at a set temperature for a certain time to obtain the MoO2 and Mn2P2O7 mixed material. According to the preparation method, 1-butyl-3-methylimidazole bis (trifluoromethane) sulfimide is used as a reaction solvent for preparing a MoO2 and Mn2P2O7 mixed material, 1-butyl-3-methylimidazole bis (trifluoromethane) sulfimide is used as an ionic liquid, and due to the low volatility of 1-butyl-3-methylimidazole bis (trifluoromethane) sulfimide, the MoO2 and Mn2P2O7 mixed material can be obtained; the problem of poor safety caused by high pressure of a closed container due to continuous volatilization of water in a hydrothermal method can be solved, so tha |
---|