Continuous casting method for eliminating netted cracks of Ni-free 09CrCuSb steel casting blank

The invention relates to a continuous casting method for eliminating netted cracks of a Ni-free 09CrCuSb steel casting blank. The steel comprises the following chemical components in percentage by weight: 0.06%-0.10% of C, 0.20%-0.35% of Si, 0.45%-0.60% of Mn, less than or equal to 0.020% of P, less...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: JIANG SHUANGHAI, DU CHENGJIAN, WANG JUN, SHI WEINING, YUAN YUAN, FANG YU, WANG LIU, XU JIYOU, YANG BEI, YE MINGZAI
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator JIANG SHUANGHAI
DU CHENGJIAN
WANG JUN
SHI WEINING
YUAN YUAN
FANG YU
WANG LIU
XU JIYOU
YANG BEI
YE MINGZAI
description The invention relates to a continuous casting method for eliminating netted cracks of a Ni-free 09CrCuSb steel casting blank. The steel comprises the following chemical components in percentage by weight: 0.06%-0.10% of C, 0.20%-0.35% of Si, 0.45%-0.60% of Mn, less than or equal to 0.020% of P, less than or equal to 0.010% of S, 0.80%-1.00% of Cr, 0.25%-0.35% of Cu and 0.04%-0.10% of Sb. The method comprises the key process steps that (1) when molten steel flows into a crystallizer from a tundish, the water volume of the crystallizer is controlled to be 158 t/h to 160 t/h, and the electromagnetic stirring parameters of the crystallizer are that the current is 450 A, and the frequency is 3 Hz; (2) when a casting blank continuously cast from the crystallizer enters a secondary cooling chamber, the secondary cooling specific water flow is 1.19-1.21; and (3) when the casting blank pulled out of the secondary cooling chamber enters a withdrawal and straightening machine, the blank temperature range of the casting
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN115627421A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN115627421A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN115627421A3</originalsourceid><addsrcrecordid>eNqNjL0KwjAURrM4iPoO1wcomPqHowTFqYvuIU1vNDTNLbnJ-1tEnJ3Ox-HjzIVWFLOPhQqDNTzNJwyYX9SBowQY_OCj-eiIOWMHNhnbM5CDxlcuIcLmpJIq9xY4I4Zfpg0m9ksxcyYwrr5ciPX18lC3CkfSyKOxOHW1aqTcH-rjrpbn7T-fNz1LPCg</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Continuous casting method for eliminating netted cracks of Ni-free 09CrCuSb steel casting blank</title><source>esp@cenet</source><creator>JIANG SHUANGHAI ; DU CHENGJIAN ; WANG JUN ; SHI WEINING ; YUAN YUAN ; FANG YU ; WANG LIU ; XU JIYOU ; YANG BEI ; YE MINGZAI</creator><creatorcontrib>JIANG SHUANGHAI ; DU CHENGJIAN ; WANG JUN ; SHI WEINING ; YUAN YUAN ; FANG YU ; WANG LIU ; XU JIYOU ; YANG BEI ; YE MINGZAI</creatorcontrib><description>The invention relates to a continuous casting method for eliminating netted cracks of a Ni-free 09CrCuSb steel casting blank. The steel comprises the following chemical components in percentage by weight: 0.06%-0.10% of C, 0.20%-0.35% of Si, 0.45%-0.60% of Mn, less than or equal to 0.020% of P, less than or equal to 0.010% of S, 0.80%-1.00% of Cr, 0.25%-0.35% of Cu and 0.04%-0.10% of Sb. The method comprises the key process steps that (1) when molten steel flows into a crystallizer from a tundish, the water volume of the crystallizer is controlled to be 158 t/h to 160 t/h, and the electromagnetic stirring parameters of the crystallizer are that the current is 450 A, and the frequency is 3 Hz; (2) when a casting blank continuously cast from the crystallizer enters a secondary cooling chamber, the secondary cooling specific water flow is 1.19-1.21; and (3) when the casting blank pulled out of the secondary cooling chamber enters a withdrawal and straightening machine, the blank temperature range of the casting</description><language>chi ; eng</language><subject>ALLOYS ; CASTING ; CASTING OF METALS ; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES ; CHEMISTRY ; FERROUS OR NON-FERROUS ALLOYS ; METALLURGY ; PERFORMING OPERATIONS ; POWDER METALLURGY ; TRANSPORTING ; TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><creationdate>2023</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20230120&amp;DB=EPODOC&amp;CC=CN&amp;NR=115627421A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,778,883,25551,76304</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20230120&amp;DB=EPODOC&amp;CC=CN&amp;NR=115627421A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>JIANG SHUANGHAI</creatorcontrib><creatorcontrib>DU CHENGJIAN</creatorcontrib><creatorcontrib>WANG JUN</creatorcontrib><creatorcontrib>SHI WEINING</creatorcontrib><creatorcontrib>YUAN YUAN</creatorcontrib><creatorcontrib>FANG YU</creatorcontrib><creatorcontrib>WANG LIU</creatorcontrib><creatorcontrib>XU JIYOU</creatorcontrib><creatorcontrib>YANG BEI</creatorcontrib><creatorcontrib>YE MINGZAI</creatorcontrib><title>Continuous casting method for eliminating netted cracks of Ni-free 09CrCuSb steel casting blank</title><description>The invention relates to a continuous casting method for eliminating netted cracks of a Ni-free 09CrCuSb steel casting blank. The steel comprises the following chemical components in percentage by weight: 0.06%-0.10% of C, 0.20%-0.35% of Si, 0.45%-0.60% of Mn, less than or equal to 0.020% of P, less than or equal to 0.010% of S, 0.80%-1.00% of Cr, 0.25%-0.35% of Cu and 0.04%-0.10% of Sb. The method comprises the key process steps that (1) when molten steel flows into a crystallizer from a tundish, the water volume of the crystallizer is controlled to be 158 t/h to 160 t/h, and the electromagnetic stirring parameters of the crystallizer are that the current is 450 A, and the frequency is 3 Hz; (2) when a casting blank continuously cast from the crystallizer enters a secondary cooling chamber, the secondary cooling specific water flow is 1.19-1.21; and (3) when the casting blank pulled out of the secondary cooling chamber enters a withdrawal and straightening machine, the blank temperature range of the casting</description><subject>ALLOYS</subject><subject>CASTING</subject><subject>CASTING OF METALS</subject><subject>CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES</subject><subject>CHEMISTRY</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>METALLURGY</subject><subject>PERFORMING OPERATIONS</subject><subject>POWDER METALLURGY</subject><subject>TRANSPORTING</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2023</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNjL0KwjAURrM4iPoO1wcomPqHowTFqYvuIU1vNDTNLbnJ-1tEnJ3Ox-HjzIVWFLOPhQqDNTzNJwyYX9SBowQY_OCj-eiIOWMHNhnbM5CDxlcuIcLmpJIq9xY4I4Zfpg0m9ksxcyYwrr5ciPX18lC3CkfSyKOxOHW1aqTcH-rjrpbn7T-fNz1LPCg</recordid><startdate>20230120</startdate><enddate>20230120</enddate><creator>JIANG SHUANGHAI</creator><creator>DU CHENGJIAN</creator><creator>WANG JUN</creator><creator>SHI WEINING</creator><creator>YUAN YUAN</creator><creator>FANG YU</creator><creator>WANG LIU</creator><creator>XU JIYOU</creator><creator>YANG BEI</creator><creator>YE MINGZAI</creator><scope>EVB</scope></search><sort><creationdate>20230120</creationdate><title>Continuous casting method for eliminating netted cracks of Ni-free 09CrCuSb steel casting blank</title><author>JIANG SHUANGHAI ; DU CHENGJIAN ; WANG JUN ; SHI WEINING ; YUAN YUAN ; FANG YU ; WANG LIU ; XU JIYOU ; YANG BEI ; YE MINGZAI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN115627421A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2023</creationdate><topic>ALLOYS</topic><topic>CASTING</topic><topic>CASTING OF METALS</topic><topic>CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES</topic><topic>CHEMISTRY</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>METALLURGY</topic><topic>PERFORMING OPERATIONS</topic><topic>POWDER METALLURGY</topic><topic>TRANSPORTING</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>JIANG SHUANGHAI</creatorcontrib><creatorcontrib>DU CHENGJIAN</creatorcontrib><creatorcontrib>WANG JUN</creatorcontrib><creatorcontrib>SHI WEINING</creatorcontrib><creatorcontrib>YUAN YUAN</creatorcontrib><creatorcontrib>FANG YU</creatorcontrib><creatorcontrib>WANG LIU</creatorcontrib><creatorcontrib>XU JIYOU</creatorcontrib><creatorcontrib>YANG BEI</creatorcontrib><creatorcontrib>YE MINGZAI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>JIANG SHUANGHAI</au><au>DU CHENGJIAN</au><au>WANG JUN</au><au>SHI WEINING</au><au>YUAN YUAN</au><au>FANG YU</au><au>WANG LIU</au><au>XU JIYOU</au><au>YANG BEI</au><au>YE MINGZAI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Continuous casting method for eliminating netted cracks of Ni-free 09CrCuSb steel casting blank</title><date>2023-01-20</date><risdate>2023</risdate><abstract>The invention relates to a continuous casting method for eliminating netted cracks of a Ni-free 09CrCuSb steel casting blank. The steel comprises the following chemical components in percentage by weight: 0.06%-0.10% of C, 0.20%-0.35% of Si, 0.45%-0.60% of Mn, less than or equal to 0.020% of P, less than or equal to 0.010% of S, 0.80%-1.00% of Cr, 0.25%-0.35% of Cu and 0.04%-0.10% of Sb. The method comprises the key process steps that (1) when molten steel flows into a crystallizer from a tundish, the water volume of the crystallizer is controlled to be 158 t/h to 160 t/h, and the electromagnetic stirring parameters of the crystallizer are that the current is 450 A, and the frequency is 3 Hz; (2) when a casting blank continuously cast from the crystallizer enters a secondary cooling chamber, the secondary cooling specific water flow is 1.19-1.21; and (3) when the casting blank pulled out of the secondary cooling chamber enters a withdrawal and straightening machine, the blank temperature range of the casting</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN115627421A
source esp@cenet
subjects ALLOYS
CASTING
CASTING OF METALS
CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES
CHEMISTRY
FERROUS OR NON-FERROUS ALLOYS
METALLURGY
PERFORMING OPERATIONS
POWDER METALLURGY
TRANSPORTING
TREATMENT OF ALLOYS OR NON-FERROUS METALS
title Continuous casting method for eliminating netted cracks of Ni-free 09CrCuSb steel casting blank
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-15T12%3A55%3A29IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=JIANG%20SHUANGHAI&rft.date=2023-01-20&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN115627421A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true