Pre-hardened mirror plastic die steel and production method thereof

The invention relates to pre-hardened mirror surface plastic die steel and a production method thereof, the die steel comprises the following elements in percentage by mass: 0.20-0.25% of C, 0.50-0.70% of Si, 1.80-2.00% of Mn, less than or equal to 0.005% of S, less than or equal to 0.015% of P, 3.0...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: ZHANG KAIGUANG, ZHANG YUANPU, ZUO PEI, BU YONG, WANG XIANJUN, YANG XIULI, XI TIANHUI, YU HONGWEI
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The invention relates to pre-hardened mirror surface plastic die steel and a production method thereof, the die steel comprises the following elements in percentage by mass: 0.20-0.25% of C, 0.50-0.70% of Si, 1.80-2.00% of Mn, less than or equal to 0.005% of S, less than or equal to 0.015% of P, 3.0-5.0% of Cr, 0.30-0.50% of Mo, 1.00-1.50% of Ni, less than or equal to 0.01% of Al, less than or equal to 0.005% of N, 00008-0.0015% of B and the balance of Fe and inevitable impurities, and the chemical components also need to meet the following formula: (1) B = 0.043% + 0.625% of S-0. 128% of C-0.0031% of Cr-0.0036% of Mo; (2) Al is equal to-0.034% to 0.167% of C, 5.69% of S, 0.696% of Ti and 9.87% of N; the production method comprises the steps of KR desulfurizer-130t converter-LF-RH-slab continuous casting, casting blank heating, rolling, normalizing heat treatment and tempering heat treatment. The Rockwell hardness HRC28-34 of the manufactured extra-thick steel plate for the plastic mold is HRC28-34, the maxim