Leather non-pickling salt-free high-absorption chrome tanning process method
The invention provides a non-pickling salt-free high-absorption chrome tanning process method for leather. The method comprises the following steps: step 1, weighing and metering; step 2, soaking in water; step 3, liming; step 4, washing with water; step 5, pre-deliming; step 6, deliming and softeni...
Gespeichert in:
Hauptverfasser: | , , , , |
---|---|
Format: | Patent |
Sprache: | chi ; eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | The invention provides a non-pickling salt-free high-absorption chrome tanning process method for leather. The method comprises the following steps: step 1, weighing and metering; step 2, soaking in water; step 3, liming; step 4, washing with water; step 5, pre-deliming; step 6, deliming and softening: adding 0.5-1 time of 30 DEG C water, adding 0.8% of a deliming agent and 0.2% of a degreasing agent, adding sulfuric acid to adjust the pH value to 3.5, and adding 0.5% of softening compound enzyme and 0.5% of an auxiliary agent; step 7, washing with water; step 8, chrome tanning; step 9, adding acid: adding formic acid and rotating for 30 minutes, wherein the use amount of the formic acid is 0.4-0.5% of the tare weight of the raw materials; step 10, adding acid for several times; the method has the characteristics that the production cost is saved, the environmental pollution is reduced, and the quality index of a finished product is not reduced by promoting chrome tanning absorption.
本发明提供一种皮革不浸酸无盐高吸收铬鞣工艺方法,该 |
---|