Production formula of rubber roller for Siro compact spinning
The invention provides a production formula of a rubber roller for Siro compact spinning. The rubber roller comprises an aluminum pipe roller core and a rubber composite material layer wrapping the aluminum pipe roller core. The rubber composite material layer is prepared from the following raw mate...
Gespeichert in:
Hauptverfasser: | , , , |
---|---|
Format: | Patent |
Sprache: | chi ; eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | The invention provides a production formula of a rubber roller for Siro compact spinning. The rubber roller comprises an aluminum pipe roller core and a rubber composite material layer wrapping the aluminum pipe roller core. The rubber composite material layer is prepared from the following raw material components in parts by weight: 50-70 parts of butyronitrile-isoprene rubber; 30-50 parts of carboxy nitrile rubber; 4-10 parts of AS resin; 3 parts of a functional auxiliary agent; 2-3 parts of an accelerant; 5 parts of zinc oxide; 2-5 parts of an antistatic lubricant; 8 parts of titanium dioxide; 1 part of stearic acid; 2 parts of an anti-aging agent; 5-9 parts of a plasticizer DINP; 3-6 parts of a reinforcing agent; and 6-10 parts of colloidal sulfur. According to the production formula of the rubber roller for Siro compact spinning, quaternary blending modified rubber is used as a main body material, so that the properties including static electricity resistance, tear resistance, wear resistance and swellin |
---|