Asphalt/cement composite-based normal-temperature self-compacting asphalt concrete and preparation method thereof

The invention discloses asphalt/cement composite-based normal-temperature self-compacting asphalt concrete. The asphalt/cement composite-based normal-temperature self-compacting asphalt concrete comprises the following components in parts by weight: 10-20 parts of emulsified asphalt, 4-12 parts of c...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: HUANG ZHENGHONG, HUANG TIANJUN, FENG JIANLIN, WU FAN, DOU YANZHU, CHEN ANQI, XIE JUNKAI, BAI TAO, GUAN SHIYU, LI YUANYUAN, MAO CHUNGUANG
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The invention discloses asphalt/cement composite-based normal-temperature self-compacting asphalt concrete. The asphalt/cement composite-based normal-temperature self-compacting asphalt concrete comprises the following components in parts by weight: 10-20 parts of emulsified asphalt, 4-12 parts of cement, 40-73 parts of aggregate, 12-23 parts of mineral powder, 1-3 parts of a bonding agent and 1-5 parts of water. By optimizing the formula and grading composition of the asphalt concrete, the obtained concrete can be mixed and paved at normal temperature, can realize self-compaction (without being rolled by a compaction machine) after being paved, and shows the advantages of high early strength and the like; and the related preparation and construction methods are relatively simple, environment-friendly, low in energy consumption and suitable for popularization and application. 本发明公开了一种沥青/水泥复合基常温自密实沥青混凝土,各组分及其所占重量份数包括:乳化沥青10~20份,水泥4~12份,集料40~73份、矿粉12~23份,键合剂1~3份,水1~5份。本发明通过对沥青混凝土配方和级配组成进行优化,所得混凝土可进行常温拌和、摊铺,摊铺后能