Method for recovering multi-metal crystals and co-producing water glass from copper-nickel sulfide ore tailings

The invention relates to a method for recovering multi-metal crystals and co-producing water glass from copper-nickel sulfide ore tailings, the method comprises the following steps: S1, mixing the copper-nickel sulfide ore tailings and an auxiliary agent according to a mass ratio of 1: (0.5-2), grin...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: PAN AIFANG, MA RUNYONG, MA YUZHAO, SUN YUE
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator PAN AIFANG
MA RUNYONG
MA YUZHAO
SUN YUE
description The invention relates to a method for recovering multi-metal crystals and co-producing water glass from copper-nickel sulfide ore tailings, the method comprises the following steps: S1, mixing the copper-nickel sulfide ore tailings and an auxiliary agent according to a mass ratio of 1: (0.5-2), grinding to 200-300 meshes, carrying out aerobic roasting to obtain active clinker, and collecting furnace gas generated by roasting; the additive is sodium hydroxide or sodium carbonate; s2, leaching the active clinker with water to obtain water leaching residues and water leaching liquid containing sodium silicate; s3, carrying out carbonation decomposition on the water immersion liquid to obtain silica gel and Na2CO3 filtrate, wherein the Na2CO3 filtrate is used for S1; s4, fully oxidizing the furnace gas, collecting with water to obtain a sulfuric acid solution, adjusting the concentration to 1-6 mol/L, and leaching the water leaching residues to obtain acid leaching residues and a first filtrate; s5, heating and a
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN113830776A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN113830776A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN113830776A3</originalsourceid><addsrcrecordid>eNqNjEEKwjAQRbtxIeodxgMELAXrVoriRlfuS0gmNTTNhJlU8fZG8ACu3uK_95cVXTE_yIIjBkZDT2QfB5jmkL2aMOsAht9SKKCjBUMqMdnZfK2XzsgwBC0Cjmkqa0rIKnozYgCZg_MWgRghax9KIutq4coXbn5cVdvz6d5dFCbqUZI2GDH33a2um0Oza9v9sfnH-QBCJ0Nh</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Method for recovering multi-metal crystals and co-producing water glass from copper-nickel sulfide ore tailings</title><source>esp@cenet</source><creator>PAN AIFANG ; MA RUNYONG ; MA YUZHAO ; SUN YUE</creator><creatorcontrib>PAN AIFANG ; MA RUNYONG ; MA YUZHAO ; SUN YUE</creatorcontrib><description>The invention relates to a method for recovering multi-metal crystals and co-producing water glass from copper-nickel sulfide ore tailings, the method comprises the following steps: S1, mixing the copper-nickel sulfide ore tailings and an auxiliary agent according to a mass ratio of 1: (0.5-2), grinding to 200-300 meshes, carrying out aerobic roasting to obtain active clinker, and collecting furnace gas generated by roasting; the additive is sodium hydroxide or sodium carbonate; s2, leaching the active clinker with water to obtain water leaching residues and water leaching liquid containing sodium silicate; s3, carrying out carbonation decomposition on the water immersion liquid to obtain silica gel and Na2CO3 filtrate, wherein the Na2CO3 filtrate is used for S1; s4, fully oxidizing the furnace gas, collecting with water to obtain a sulfuric acid solution, adjusting the concentration to 1-6 mol/L, and leaching the water leaching residues to obtain acid leaching residues and a first filtrate; s5, heating and a</description><language>chi ; eng</language><subject>CHEMISTRY ; COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F ; COMPOUNDS OF THE METALS BERYLLIUM, MAGNESIUM, ALUMINIUM,CALCIUM, STRONTIUM, BARIUM, RADIUM, THORIUM, OR OF THERARE-EARTH METALS ; COMPOUNDS THEREOF ; INORGANIC CHEMISTRY ; METALLURGY ; NON-METALLIC ELEMENTS</subject><creationdate>2021</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20211224&amp;DB=EPODOC&amp;CC=CN&amp;NR=113830776A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25543,76293</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20211224&amp;DB=EPODOC&amp;CC=CN&amp;NR=113830776A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>PAN AIFANG</creatorcontrib><creatorcontrib>MA RUNYONG</creatorcontrib><creatorcontrib>MA YUZHAO</creatorcontrib><creatorcontrib>SUN YUE</creatorcontrib><title>Method for recovering multi-metal crystals and co-producing water glass from copper-nickel sulfide ore tailings</title><description>The invention relates to a method for recovering multi-metal crystals and co-producing water glass from copper-nickel sulfide ore tailings, the method comprises the following steps: S1, mixing the copper-nickel sulfide ore tailings and an auxiliary agent according to a mass ratio of 1: (0.5-2), grinding to 200-300 meshes, carrying out aerobic roasting to obtain active clinker, and collecting furnace gas generated by roasting; the additive is sodium hydroxide or sodium carbonate; s2, leaching the active clinker with water to obtain water leaching residues and water leaching liquid containing sodium silicate; s3, carrying out carbonation decomposition on the water immersion liquid to obtain silica gel and Na2CO3 filtrate, wherein the Na2CO3 filtrate is used for S1; s4, fully oxidizing the furnace gas, collecting with water to obtain a sulfuric acid solution, adjusting the concentration to 1-6 mol/L, and leaching the water leaching residues to obtain acid leaching residues and a first filtrate; s5, heating and a</description><subject>CHEMISTRY</subject><subject>COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F</subject><subject>COMPOUNDS OF THE METALS BERYLLIUM, MAGNESIUM, ALUMINIUM,CALCIUM, STRONTIUM, BARIUM, RADIUM, THORIUM, OR OF THERARE-EARTH METALS</subject><subject>COMPOUNDS THEREOF</subject><subject>INORGANIC CHEMISTRY</subject><subject>METALLURGY</subject><subject>NON-METALLIC ELEMENTS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2021</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNjEEKwjAQRbtxIeodxgMELAXrVoriRlfuS0gmNTTNhJlU8fZG8ACu3uK_95cVXTE_yIIjBkZDT2QfB5jmkL2aMOsAht9SKKCjBUMqMdnZfK2XzsgwBC0Cjmkqa0rIKnozYgCZg_MWgRghax9KIutq4coXbn5cVdvz6d5dFCbqUZI2GDH33a2um0Oza9v9sfnH-QBCJ0Nh</recordid><startdate>20211224</startdate><enddate>20211224</enddate><creator>PAN AIFANG</creator><creator>MA RUNYONG</creator><creator>MA YUZHAO</creator><creator>SUN YUE</creator><scope>EVB</scope></search><sort><creationdate>20211224</creationdate><title>Method for recovering multi-metal crystals and co-producing water glass from copper-nickel sulfide ore tailings</title><author>PAN AIFANG ; MA RUNYONG ; MA YUZHAO ; SUN YUE</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN113830776A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2021</creationdate><topic>CHEMISTRY</topic><topic>COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F</topic><topic>COMPOUNDS OF THE METALS BERYLLIUM, MAGNESIUM, ALUMINIUM,CALCIUM, STRONTIUM, BARIUM, RADIUM, THORIUM, OR OF THERARE-EARTH METALS</topic><topic>COMPOUNDS THEREOF</topic><topic>INORGANIC CHEMISTRY</topic><topic>METALLURGY</topic><topic>NON-METALLIC ELEMENTS</topic><toplevel>online_resources</toplevel><creatorcontrib>PAN AIFANG</creatorcontrib><creatorcontrib>MA RUNYONG</creatorcontrib><creatorcontrib>MA YUZHAO</creatorcontrib><creatorcontrib>SUN YUE</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>PAN AIFANG</au><au>MA RUNYONG</au><au>MA YUZHAO</au><au>SUN YUE</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Method for recovering multi-metal crystals and co-producing water glass from copper-nickel sulfide ore tailings</title><date>2021-12-24</date><risdate>2021</risdate><abstract>The invention relates to a method for recovering multi-metal crystals and co-producing water glass from copper-nickel sulfide ore tailings, the method comprises the following steps: S1, mixing the copper-nickel sulfide ore tailings and an auxiliary agent according to a mass ratio of 1: (0.5-2), grinding to 200-300 meshes, carrying out aerobic roasting to obtain active clinker, and collecting furnace gas generated by roasting; the additive is sodium hydroxide or sodium carbonate; s2, leaching the active clinker with water to obtain water leaching residues and water leaching liquid containing sodium silicate; s3, carrying out carbonation decomposition on the water immersion liquid to obtain silica gel and Na2CO3 filtrate, wherein the Na2CO3 filtrate is used for S1; s4, fully oxidizing the furnace gas, collecting with water to obtain a sulfuric acid solution, adjusting the concentration to 1-6 mol/L, and leaching the water leaching residues to obtain acid leaching residues and a first filtrate; s5, heating and a</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN113830776A
source esp@cenet
subjects CHEMISTRY
COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F
COMPOUNDS OF THE METALS BERYLLIUM, MAGNESIUM, ALUMINIUM,CALCIUM, STRONTIUM, BARIUM, RADIUM, THORIUM, OR OF THERARE-EARTH METALS
COMPOUNDS THEREOF
INORGANIC CHEMISTRY
METALLURGY
NON-METALLIC ELEMENTS
title Method for recovering multi-metal crystals and co-producing water glass from copper-nickel sulfide ore tailings
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-23T20%3A01%3A41IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=PAN%20AIFANG&rft.date=2021-12-24&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN113830776A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true