Method for recovering multi-metal crystals and co-producing water glass from copper-nickel sulfide ore tailings
The invention relates to a method for recovering multi-metal crystals and co-producing water glass from copper-nickel sulfide ore tailings, the method comprises the following steps: S1, mixing the copper-nickel sulfide ore tailings and an auxiliary agent according to a mass ratio of 1: (0.5-2), grin...
Gespeichert in:
Hauptverfasser: | , , , |
---|---|
Format: | Patent |
Sprache: | chi ; eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | The invention relates to a method for recovering multi-metal crystals and co-producing water glass from copper-nickel sulfide ore tailings, the method comprises the following steps: S1, mixing the copper-nickel sulfide ore tailings and an auxiliary agent according to a mass ratio of 1: (0.5-2), grinding to 200-300 meshes, carrying out aerobic roasting to obtain active clinker, and collecting furnace gas generated by roasting; the additive is sodium hydroxide or sodium carbonate; s2, leaching the active clinker with water to obtain water leaching residues and water leaching liquid containing sodium silicate; s3, carrying out carbonation decomposition on the water immersion liquid to obtain silica gel and Na2CO3 filtrate, wherein the Na2CO3 filtrate is used for S1; s4, fully oxidizing the furnace gas, collecting with water to obtain a sulfuric acid solution, adjusting the concentration to 1-6 mol/L, and leaching the water leaching residues to obtain acid leaching residues and a first filtrate; s5, heating and a |
---|