POLYETHYLENE YARN, METHOD FOR MANUFACTURING SAME, AND COOL-FEELING FABRIC COMPRISING SAME

Disclosed are polyethylene yarn, a method for manufacturing same, and a cool-feeling fabric comprising same, wherein the polyethylene yarn has improved weavability to enable the manufacturing of the cool-feeling fabric that can provide a user with soft tactile sensation as well as cooling sensation...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: LEE SIN-HO, LEE SANG-MOK, KIM JAE-HYEONG, LEE YOUNG-SOO, KIM SONG-RYONG, KIM GI-WOONG
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Disclosed are polyethylene yarn, a method for manufacturing same, and a cool-feeling fabric comprising same, wherein the polyethylene yarn has improved weavability to enable the manufacturing of the cool-feeling fabric that can provide a user with soft tactile sensation as well as cooling sensation and has excellent pilling resistance, abrasion resistance, cuttability, and sewability. In a stress-strain curve of the polyethylene yarn, obtained from the measurement at room temperature, (i) the elongation is 0.5 to 3% at a stress of 1 g/d, (ii) the elongation is 5.5 to 10% at a stress of 3 g/d, and (iii) the difference between the elongation at a stress of 4 g/d and the elongation at the maximum stress is 5.5 to 25%, wherein the polyethylene yarn has a toughness of 55 to 120 J/m at room temperature. 公开了一种聚乙烯纱线、该聚乙烯纱线的制造方法及包括该聚乙烯纱线的皮肤冷却织物,其中该聚乙烯纱线具有提高的可编织性并且能够制造能为使用者提供柔软触感及凉感并且具有优异的抗起球性、耐磨性、可裁剪性及可缝纫性的皮肤冷却织物。在室温下测量获得的该聚乙烯纱线的强度-伸长率曲线中,(i)在1g/d的强度下的伸长率为0.5%至3%,(ii)在3g/d的强度下的伸长率为5.5%至10%,(iii)在4g/d的强度下的伸长率与在最大强度下的伸长