Process for laser cladding of nickel-based tungsten carbide on copper alloy core glass mold
The invention relates to a process for laser cladding of nickel-based tungsten carbide for a copper alloy core glass mold. The process comprises the following steps that A, machining turning is carried out on a copper alloy core to obtain a workpiece before cladding; B, laser cladding pre-treatment...
Gespeichert in:
1. Verfasser: | |
---|---|
Format: | Patent |
Sprache: | chi ; eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | The invention relates to a process for laser cladding of nickel-based tungsten carbide for a copper alloy core glass mold. The process comprises the following steps that A, machining turning is carried out on a copper alloy core to obtain a workpiece before cladding; B, laser cladding pre-treatment is carried out, specifically, oil stains and dust on the surface of the core are cleaned; C, a track program is programmed; D, laser cladding is carried out, specifically, technological parameters are set, laser cladding is carried out along a program track, and adopted nickel-based tungsten carbide alloy powder comprises the following components of, 1.28% of B, 2.38% of C, 4.37% of Co, 7.63% of Cr, 2.04% of Fe, 2.34% of Si, 31.06% of W and the balance Ni.
本发明涉及一种铜合金芯子玻璃模具激光熔覆镍基碳化钨工艺;包括以下步骤:A)对铜合金芯子进行机加工车削,获得熔覆前工件;B)激光熔覆前道处理:清洁芯子表面油污及粉尘;C)编程轨迹程序;D)激光熔覆:设定好工艺参数,沿着程序轨迹进行激光熔覆。所采用的镍基碳化钨合金粉成分为B:1.28%,C:2.38%,Co:4.37%,Cr:7.63%,Fe:2.04%,Si:2.34%,W:31.06%,其余均为Ni。 |
---|