Sodium silicate concrete and preparation method thereof

The invention discloses sodium silicate concrete and a preparation method thereof. The sodium silicate concrete is prepared from the following raw materials in parts by weight: 200 to 300 parts of cement, 160 to 180 parts of water glass, 60 to 80 parts of sodium fluosilicate, 70 to 90 parts of magne...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
1. Verfasser: YANG RONGFEI
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The invention discloses sodium silicate concrete and a preparation method thereof. The sodium silicate concrete is prepared from the following raw materials in parts by weight: 200 to 300 parts of cement, 160 to 180 parts of water glass, 60 to 80 parts of sodium fluosilicate, 70 to 90 parts of magnesium hydroxide, 200 to 260 parts of quartz powder, 5 to 9 parts of quartz sand, 2.8 to 4.2 parts of quartzite, 30 to 40 parts of chloroprene rubber, 5 to 10 parts of synthetic resin, 5 to 8 parts of a water reducing agent, 3.2 to 4.6 parts of a synergist and 60 to 70 parts of water. According to the present invention, the design is novel, the CTF synergist, the LBD synergist and the water reducing agent are added to the concrete so that the inorganic insoluble particles in the concrete can be well dispersed, the synthetic resin can increase the viscosity of the stirred material and ensure the corrosion resistance of the concrete after the solidification, and the added chloroprene rubber belongs to the synthetic rub