Reactive powder concrete and preparation method thereof

The invention relates to reactive powder concrete and a preparation method thereof. The reactive powder concrete comprises the following components: 28%-32% of cement, 7%-8% of a mineral admixture, 45%-50% of mixed quartz sand, 1%-2% of a water reducing agent, 5%-6% of steel fibers and the balance o...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: TANG YINXIA, JIANG XIANGDONG
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The invention relates to reactive powder concrete and a preparation method thereof. The reactive powder concrete comprises the following components: 28%-32% of cement, 7%-8% of a mineral admixture, 45%-50% of mixed quartz sand, 1%-2% of a water reducing agent, 5%-6% of steel fibers and the balance of water, the mineral admixture is I-grade fine ground slag; the mixed quartz sand comprises the following components: 40-45% of coarse-particle-size quartz sand, 30-35% of medium-particle-size quartz sand and 24-28% of fine-particle-size quartz sand; the preparation method comprises the following steps: pre-stirring mixed quartz sand and steel fiber for 60 seconds, adding cement, a mineral admixture, a water reducing agent and water, and stirring for 2-3 minutes to obtain reactive powder concrete; the cement, the mineral admixture and other active powder materials are used as main materials, and the mixed quartz sand, the water reducing agent, the steel fiber and the water are used as auxiliary materials, so that t