Preparation method of Bi-MoS2 nano composite material for electrocatalytic synthesis of ammonia
The invention relates to a preparation method of a Bi-MoS2 nano composite material for electrocatalytic synthesis of ammonia, and belongs to the technical field of nano materials. The Bi-MoS2 nanocomposite takes molybdenum disulfide as a substrate, and bismuth nanocrystals are compounded on the moly...
Gespeichert in:
Hauptverfasser: | , , , , , , |
---|---|
Format: | Patent |
Sprache: | chi ; eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | The invention relates to a preparation method of a Bi-MoS2 nano composite material for electrocatalytic synthesis of ammonia, and belongs to the technical field of nano materials. The Bi-MoS2 nanocomposite takes molybdenum disulfide as a substrate, and bismuth nanocrystals are compounded on the molybdenum disulfide substrate; molybdenum disulfide is used as a substrate, and bismuth nanocrystals and molybdenum disulfide nanosheets are compounded through a hydrothermal reaction. The preparation process is simple and feasible, low in cost and environment-friendly, excellent electrochemical activity can be shown under the condition that precious metal is not utilized, the ammonia yield can reach 15 microgram h mg cat, and the Faraday efficiency can reach 25%.
本发明涉及一种用于电催化合成氨的Bi-MoS2纳米复合材料的制备方法,属于纳米材料技术领域;所述Bi-MoS2纳米复合材料以二硫化钼为基底,铋纳米晶体复合在二硫化钼基底上;以二硫化钼为基底,通过水热反应将铋纳米晶体与二硫化钼纳米片进行复合。本发明的制备过程简单可行,成本低廉且对环境友好,在不利用贵金属的条件下能够表现出优异的电化学活性,氨产率可达~15μg h-1mg-1cat,法拉第效率可达~25%。 |
---|