Preparation method of low-volume-shrinkage carbon nanofiber aerogel
The invention relates to a preparation method of low-volume-shrinkage carbon nanofiber aerogel. The preparation method comprises the following steps of: preparing polymer nanofibers through electrostatic spinning; carrying out stabilization and carbonization treatment to obtain carbon nanofibers; pr...
Gespeichert in:
Hauptverfasser: | , , , , , |
---|---|
Format: | Patent |
Sprache: | chi ; eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | The invention relates to a preparation method of low-volume-shrinkage carbon nanofiber aerogel. The preparation method comprises the following steps of: preparing polymer nanofibers through electrostatic spinning; carrying out stabilization and carbonization treatment to obtain carbon nanofibers; preparing a carbon nanofiber aqueous dispersion through homogenate dispersion, and then carrying out freeze forming and freeze drying on the carbon nanofiber aqueous dispersion to obtain aerogel; and then carrying out thermal crosslinking and pyrolysis treatment or only carrying out pyrolysis treatment. According to the preparation method disclosed by the invention, by means of a mode of sequentially carrying out carbonization, pyrolysis and auxiliary agent-assisted regulation and control, the obtained aerogel material has good mechanical property and low volume shrinkage; and the problems of high brittleness and high volume shrinkage of carbon nanofiber aerogel prepared by traditional electrostatic spinning are impr |
---|