Self-repairing cement for thermal damage tunnel

The invention relates to the technical field of building materials, in particular to self-repairing cement for a thermal damage tunnel, the self-repairing cement is prepared from the following raw materials in percentage by mass: 67-89.5% of component A, 10-20% of component B, 0-10% of clay brick po...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: DONG HUAIZHENG, LI YONGLIANG, ZHENG CHANGQING, WANG NING, HE QIANG, TAN YONGJIE, ZHONG WEN, WANG KAIYUN, LIU JIANGUANG, LIU MINGJUN, LIN YAN, FAN YOUYIN, XU YIGANG, XIA YANQING, TENG YINJIAN, WANG JIANSHENG
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The invention relates to the technical field of building materials, in particular to self-repairing cement for a thermal damage tunnel, the self-repairing cement is prepared from the following raw materials in percentage by mass: 67-89.5% of component A, 10-20% of component B, 0-10% of clay brick powder, 0.5-2% of CaCO3 whisker and 0-1% of water-retaining agent; each of the component A and the component B comprises 90-95% of self-repairing cement clinker and 5-10% of dihydrate gypsum; the self-repairing cement clinker is prepared from 20-30% of C3S, 35-55% of C2S, 1-3% of C3A, 17-26% of C4AF and 4-8% of MgO; the size of periclase in the self-repairing cement clinker of the component A is less than 1 [mu] m; the size of periclase in the self-repairing cement clinker of the component B is 35 [mu] m, and the particle size of 47-69% of the component B is greater than 65 [mu] m. Through the self-repairing cement, the problems of early structural damage, wide later cracks and poor durability of lining concrete can