Flexible comb-shaped semi-dry electrode and preparation method thereof

The invention discloses a flexible comb-shaped semi-dry electrode and a preparation method thereof. The flexible comb-shaped semi-dry electrode is prepared based on a sensitive material. the preparation method of the sensitive material comprises the following steps: uniformly mixing copper salt, a c...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: LIU YINGTAO, DU PU, LI CUIPING, LI PENGHAI, XU HAN, HUANG JUANJUAN, MENG YANYUN, LI XUEQING, SU JIANXIAN, WANG CHEN, YIN CAN, LIU CONG, GUO HAIMING, LI MINGJI, LI HONGJI
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The invention discloses a flexible comb-shaped semi-dry electrode and a preparation method thereof. The flexible comb-shaped semi-dry electrode is prepared based on a sensitive material. the preparation method of the sensitive material comprises the following steps: uniformly mixing copper salt, a carbon conductive material and titanium dioxide nano powder, then uniformly mixing with PDMS (polydimethylsiloxane), and keeping the constant temperature of 60-80 DEG C for 2-8 hours or stably placing the sensitive material in a natural room temperature state for 2-4 days to obtain the sensitive material.The sensitive material is based on the PDMS, a wet electrode or a semi-dry electrode has good flexibility, and discomfort cannot be caused to a testee. A conductive net is constructed by adopting a carbon conductive material, polarization potential is reduced by adopting titanium dioxide nano powder, an electrolyte adsorption and desorption porous structure is constructed by adopting copper salt, and the manufacture