ECTFE melt-blown film and preparation method thereof

The invention discloses an ECTFE melt-blown film and a preparation method thereof. The melt-blown film is composed of superfine fibers with the diameter of 0.1 [mu] m-5 [mu] m; and the aperture of at least 60% of the melt-blown film is 0.3 [mu] m-0. 7 [mu] m, the aperture of less than 20% of the mel...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: DAI ZHEZHEN, YU SUYUN, LIU HUI, GAO LINNA, ZHANG YANZHONG
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The invention discloses an ECTFE melt-blown film and a preparation method thereof. The melt-blown film is composed of superfine fibers with the diameter of 0.1 [mu] m-5 [mu] m; and the aperture of at least 60% of the melt-blown film is 0.3 [mu] m-0. 7 [mu] m, the aperture of less than 20% of the melt-blown film is 0.1 [mu] m-0. 3 [mu] m, and the aperture of less than 20% of the melt-blown film is 0.7 [mu] m-1. 0 [mu] m. The melt-blown film disclosed by the invention has the advantages of high tensile strength, high elongation at break, small average pore size, high filtering precision, suitability for high-temperature-resistant, acid-base-resistant and corrosion-resistant environments and the like. 本发明公开了一种ECTFE熔喷膜及其制备方法,所述熔喷膜由直径为0.1μm~5μm的超细纤维组成,至少60%的所述熔喷膜的孔径在0.3μm~0.7μm之间,小于20%的所述熔喷膜的孔径在0.1μm~0.3μm之间,小于20%的所述熔喷膜的孔径在0.7μm~1.0μm之间。本发明的熔喷膜具有拉伸强度大,断裂伸长率高,平均孔径小,过滤精度高,适用于耐高温、耐酸碱及耐腐蚀环境等优点。