Method of making wear-resisting refractory-material dies

Metallic abrasive dust from relevant industrial prodn is first treated at 300-1,300 deg.C to remove SiO2 and other non-ferromagnetic substances, then melted in middle-freq induction furnace to produce die blank and finally heat-treated at 800-1,300 deg.C to obtain required die. The said die thus pro...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: LEI JISHOU, LEI HONGQIN, GU YANWEI
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Metallic abrasive dust from relevant industrial prodn is first treated at 300-1,300 deg.C to remove SiO2 and other non-ferromagnetic substances, then melted in middle-freq induction furnace to produce die blank and finally heat-treated at 800-1,300 deg.C to obtain required die. The said die thus produced has long service life and high quality.