Method for reducing Al2O3 inclusion of low-carbon aluminum killed steel in RH single-connection process

The invention discloses a steelmaking method for reducing Al2O3 inclusion of low-carbon aluminum killed steel by adopting an RH single-connection process. The process route adopting the RH single-connection process comprises the following steps of KR molten iron pretreatment, converter treatment, RH...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: YANG GUILING, JIA CHONGXUE, ZHANG YINGJIE, SHAN XIUYING, LIU CAIFENG, GUO CHAOHAI, LI HAIFENG, YU SHUANG, HU HUADONG, WANG NANHUI, CHEN HUI, LI XIANGQIAN, XIA JINIAN, LIANG YA
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator YANG GUILING
JIA CHONGXUE
ZHANG YINGJIE
SHAN XIUYING
LIU CAIFENG
GUO CHAOHAI
LI HAIFENG
YU SHUANG
HU HUADONG
WANG NANHUI
CHEN HUI
LI XIANGQIAN
XIA JINIAN
LIANG YA
description The invention discloses a steelmaking method for reducing Al2O3 inclusion of low-carbon aluminum killed steel by adopting an RH single-connection process. The process route adopting the RH single-connection process comprises the following steps of KR molten iron pretreatment, converter treatment, RH treatment and continuous casting, so that an LE process is omitted; the process comprises the following steps of 1) optimizing a converter blowing process and a tapping process; 2) reducing the carbon and oxygen deposition and oxygen content of converter end point molten steel and the converter tapping slag amount; 3) optimizing a ladle top slag modification process; 4) optimizing the RH treatment process; and 5) optimizing continuous casting process. According to the method, the oxygen content in the steel slag is reduced, and the generation amount of Al2O3 inclusions is reduced; the generated Al2O3 is removed from the steel as much as possible; and molten steel with high inclusion content is prevented from formi
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN112626312A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN112626312A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN112626312A3</originalsourceid><addsrcrecordid>eNqNi8EKgkAQQL10iOofpg_w4AreRQovFUR32cZRl8Yd2dml38-gD-j0ePDeNhsvFCfpYZAAgfqEzo9Qs7mV4DxyUiceZACWd442PFeznGbn0wwvx0w9aCTitYZ7C7ruTDmK94Tx-y5BkFT32WawrHT4cZcdz6dH0-a0SEe6WCRPsWuuRWEqU5WFqct_mg8wcD8e</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Method for reducing Al2O3 inclusion of low-carbon aluminum killed steel in RH single-connection process</title><source>esp@cenet</source><creator>YANG GUILING ; JIA CHONGXUE ; ZHANG YINGJIE ; SHAN XIUYING ; LIU CAIFENG ; GUO CHAOHAI ; LI HAIFENG ; YU SHUANG ; HU HUADONG ; WANG NANHUI ; CHEN HUI ; LI XIANGQIAN ; XIA JINIAN ; LIANG YA</creator><creatorcontrib>YANG GUILING ; JIA CHONGXUE ; ZHANG YINGJIE ; SHAN XIUYING ; LIU CAIFENG ; GUO CHAOHAI ; LI HAIFENG ; YU SHUANG ; HU HUADONG ; WANG NANHUI ; CHEN HUI ; LI XIANGQIAN ; XIA JINIAN ; LIANG YA</creatorcontrib><description>The invention discloses a steelmaking method for reducing Al2O3 inclusion of low-carbon aluminum killed steel by adopting an RH single-connection process. The process route adopting the RH single-connection process comprises the following steps of KR molten iron pretreatment, converter treatment, RH treatment and continuous casting, so that an LE process is omitted; the process comprises the following steps of 1) optimizing a converter blowing process and a tapping process; 2) reducing the carbon and oxygen deposition and oxygen content of converter end point molten steel and the converter tapping slag amount; 3) optimizing a ladle top slag modification process; 4) optimizing the RH treatment process; and 5) optimizing continuous casting process. According to the method, the oxygen content in the steel slag is reduced, and the generation amount of Al2O3 inclusions is reduced; the generated Al2O3 is removed from the steel as much as possible; and molten steel with high inclusion content is prevented from formi</description><language>chi ; eng</language><subject>CHEMISTRY ; METALLURGY ; METALLURGY OF IRON ; PROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OFWROUGHT-IRON OR STEEL ; TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS</subject><creationdate>2021</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20210409&amp;DB=EPODOC&amp;CC=CN&amp;NR=112626312A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25543,76293</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20210409&amp;DB=EPODOC&amp;CC=CN&amp;NR=112626312A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>YANG GUILING</creatorcontrib><creatorcontrib>JIA CHONGXUE</creatorcontrib><creatorcontrib>ZHANG YINGJIE</creatorcontrib><creatorcontrib>SHAN XIUYING</creatorcontrib><creatorcontrib>LIU CAIFENG</creatorcontrib><creatorcontrib>GUO CHAOHAI</creatorcontrib><creatorcontrib>LI HAIFENG</creatorcontrib><creatorcontrib>YU SHUANG</creatorcontrib><creatorcontrib>HU HUADONG</creatorcontrib><creatorcontrib>WANG NANHUI</creatorcontrib><creatorcontrib>CHEN HUI</creatorcontrib><creatorcontrib>LI XIANGQIAN</creatorcontrib><creatorcontrib>XIA JINIAN</creatorcontrib><creatorcontrib>LIANG YA</creatorcontrib><title>Method for reducing Al2O3 inclusion of low-carbon aluminum killed steel in RH single-connection process</title><description>The invention discloses a steelmaking method for reducing Al2O3 inclusion of low-carbon aluminum killed steel by adopting an RH single-connection process. The process route adopting the RH single-connection process comprises the following steps of KR molten iron pretreatment, converter treatment, RH treatment and continuous casting, so that an LE process is omitted; the process comprises the following steps of 1) optimizing a converter blowing process and a tapping process; 2) reducing the carbon and oxygen deposition and oxygen content of converter end point molten steel and the converter tapping slag amount; 3) optimizing a ladle top slag modification process; 4) optimizing the RH treatment process; and 5) optimizing continuous casting process. According to the method, the oxygen content in the steel slag is reduced, and the generation amount of Al2O3 inclusions is reduced; the generated Al2O3 is removed from the steel as much as possible; and molten steel with high inclusion content is prevented from formi</description><subject>CHEMISTRY</subject><subject>METALLURGY</subject><subject>METALLURGY OF IRON</subject><subject>PROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OFWROUGHT-IRON OR STEEL</subject><subject>TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2021</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNi8EKgkAQQL10iOofpg_w4AreRQovFUR32cZRl8Yd2dml38-gD-j0ePDeNhsvFCfpYZAAgfqEzo9Qs7mV4DxyUiceZACWd442PFeznGbn0wwvx0w9aCTitYZ7C7ruTDmK94Tx-y5BkFT32WawrHT4cZcdz6dH0-a0SEe6WCRPsWuuRWEqU5WFqct_mg8wcD8e</recordid><startdate>20210409</startdate><enddate>20210409</enddate><creator>YANG GUILING</creator><creator>JIA CHONGXUE</creator><creator>ZHANG YINGJIE</creator><creator>SHAN XIUYING</creator><creator>LIU CAIFENG</creator><creator>GUO CHAOHAI</creator><creator>LI HAIFENG</creator><creator>YU SHUANG</creator><creator>HU HUADONG</creator><creator>WANG NANHUI</creator><creator>CHEN HUI</creator><creator>LI XIANGQIAN</creator><creator>XIA JINIAN</creator><creator>LIANG YA</creator><scope>EVB</scope></search><sort><creationdate>20210409</creationdate><title>Method for reducing Al2O3 inclusion of low-carbon aluminum killed steel in RH single-connection process</title><author>YANG GUILING ; JIA CHONGXUE ; ZHANG YINGJIE ; SHAN XIUYING ; LIU CAIFENG ; GUO CHAOHAI ; LI HAIFENG ; YU SHUANG ; HU HUADONG ; WANG NANHUI ; CHEN HUI ; LI XIANGQIAN ; XIA JINIAN ; LIANG YA</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN112626312A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2021</creationdate><topic>CHEMISTRY</topic><topic>METALLURGY</topic><topic>METALLURGY OF IRON</topic><topic>PROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OFWROUGHT-IRON OR STEEL</topic><topic>TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS</topic><toplevel>online_resources</toplevel><creatorcontrib>YANG GUILING</creatorcontrib><creatorcontrib>JIA CHONGXUE</creatorcontrib><creatorcontrib>ZHANG YINGJIE</creatorcontrib><creatorcontrib>SHAN XIUYING</creatorcontrib><creatorcontrib>LIU CAIFENG</creatorcontrib><creatorcontrib>GUO CHAOHAI</creatorcontrib><creatorcontrib>LI HAIFENG</creatorcontrib><creatorcontrib>YU SHUANG</creatorcontrib><creatorcontrib>HU HUADONG</creatorcontrib><creatorcontrib>WANG NANHUI</creatorcontrib><creatorcontrib>CHEN HUI</creatorcontrib><creatorcontrib>LI XIANGQIAN</creatorcontrib><creatorcontrib>XIA JINIAN</creatorcontrib><creatorcontrib>LIANG YA</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>YANG GUILING</au><au>JIA CHONGXUE</au><au>ZHANG YINGJIE</au><au>SHAN XIUYING</au><au>LIU CAIFENG</au><au>GUO CHAOHAI</au><au>LI HAIFENG</au><au>YU SHUANG</au><au>HU HUADONG</au><au>WANG NANHUI</au><au>CHEN HUI</au><au>LI XIANGQIAN</au><au>XIA JINIAN</au><au>LIANG YA</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Method for reducing Al2O3 inclusion of low-carbon aluminum killed steel in RH single-connection process</title><date>2021-04-09</date><risdate>2021</risdate><abstract>The invention discloses a steelmaking method for reducing Al2O3 inclusion of low-carbon aluminum killed steel by adopting an RH single-connection process. The process route adopting the RH single-connection process comprises the following steps of KR molten iron pretreatment, converter treatment, RH treatment and continuous casting, so that an LE process is omitted; the process comprises the following steps of 1) optimizing a converter blowing process and a tapping process; 2) reducing the carbon and oxygen deposition and oxygen content of converter end point molten steel and the converter tapping slag amount; 3) optimizing a ladle top slag modification process; 4) optimizing the RH treatment process; and 5) optimizing continuous casting process. According to the method, the oxygen content in the steel slag is reduced, and the generation amount of Al2O3 inclusions is reduced; the generated Al2O3 is removed from the steel as much as possible; and molten steel with high inclusion content is prevented from formi</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN112626312A
source esp@cenet
subjects CHEMISTRY
METALLURGY
METALLURGY OF IRON
PROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OFWROUGHT-IRON OR STEEL
TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS
title Method for reducing Al2O3 inclusion of low-carbon aluminum killed steel in RH single-connection process
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-23T12%3A16%3A38IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=YANG%20GUILING&rft.date=2021-04-09&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN112626312A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true