Environment-friendly calcium silicate board produced based on slag powder and preparation method of environment-friendly calcium silicate board

The invention discloses an environment-friendly calcium silicate board produced on the basis of slag powder. The environment-friendly calcium silicate board is prepared from the following raw materials in parts by mass: 25-39 parts of slag powder, 27-41 parts of slaked lime, 20-26 parts of quartz po...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: YANG FUZENG, DUAN YONGWEI, ZHU JING, YANG MIN, XU ZHENGYANG, WANG PANPAN, ZHANG YANAN, YANG FANGFANG, WANG HUA, RAN JUNSHENG, LIU KANGLI, JU XIAO, WANG JUNLI, SHI DENGKE, LIU TAO
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The invention discloses an environment-friendly calcium silicate board produced on the basis of slag powder. The environment-friendly calcium silicate board is prepared from the following raw materials in parts by mass: 25-39 parts of slag powder, 27-41 parts of slaked lime, 20-26 parts of quartz powder and 8-14 parts of wood fibers. The preparation method comprises the following steps of: weighing the raw materials according to proportions; adding water into the wood fibers for pulping treatment; adding the weighed slag powder, slaked lime and quartz powder, uniformly mixing the materials; pouring an obtained mixture into a mold; carrying out suction filtration molding to prepare a wet blank; carrying out autoclaved curing after pre-curing; naturally cooling the wet blank after finishingthe autoclaved curing; and taking out an obtained plate from a kettle, drying the board and cutting the board to obtain the environment-friendly calcium silicate board. The slag powder and the quartzpowder are used as siliceo