High-solid-content and low-viscosity polyaspartic acid ester primer-topcoat coating suitable for high-pressure airless spraying and preparation method thereof

The invention relates to a high-solid-content and low-viscosity polyaspartic acid ester primer-topcoat coating suitable for high-pressure airless spraying and a preparation method thereof. The high-solid-content low-viscosity polyaspartic acid ester primer-topcoat coating comprises the following com...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: LIU BIN, MA YUNLI, ZHU WENKAI, RONG XUERONG, GU KEYI, WU DUANHONG, CHEN JIANGANG, HUA ZHONGLIANG, ZHONG JIANGXING, TANG SONG
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The invention relates to a high-solid-content and low-viscosity polyaspartic acid ester primer-topcoat coating suitable for high-pressure airless spraying and a preparation method thereof. The high-solid-content low-viscosity polyaspartic acid ester primer-topcoat coating comprises the following components in percentage by mass: 30-40% of polyaspartic acid ester resin; 10%-20% of polyester resin;0.3%-1.5% of a dispersing agent; 0.3%-1.0% of a defoaming agent; 1%-3% of a dehydrating agent; 0.3%-0.8% of a leveling agent; 0.4%-1.5% of an anti-sagging agent; 1%-3.0% of an ultraviolet absorber; 34%-45% of pigment; 10%-25% of a filler; 6%-10% of a solvent; 20%-29% of curing agent. Conventional high-pressure airless spraying equipment can be adopted for construction, it is guaranteed that the mixed paint can be normally constructed after 30 min at the environment temperature of 30 DEG C, the surface of a paint film is leveled normally, the defects of pinholes, shrinkage cavities, bubbles andthe like are avoided, the