Pouring process for resin matrix composite bus duct
The invention discloses a pouring process for a resin matrix composite bus duct. The pouring process comprises the following steps of: preparing a mold, and then fixing a busbar in the mold; mixing raw materials of a resin matrix composite according to a ratio at normal temperature, carrying out ult...
Gespeichert in:
Hauptverfasser: | , |
---|---|
Format: | Patent |
Sprache: | chi ; eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | CHEN DINGXUAN XIE FEI |
description | The invention discloses a pouring process for a resin matrix composite bus duct. The pouring process comprises the following steps of: preparing a mold, and then fixing a busbar in the mold; mixing raw materials of a resin matrix composite according to a ratio at normal temperature, carrying out ultrasonic treatment on the mixed materials under a negative pressure condition, and pumping out escaped foreign gas; conducting pouring under a vacuum condition; and performing curing and demolding at a constant temperature, carrying out trimming and polishing. The resin matrix composite is prepared from the following raw materials in parts by weight: 55-68 parts of epoxy resin, 10-18 parts of acrylic resin, 20-30 parts of glass fibers, 0.5-1 part of aluminum oxide, 2-5 parts of a curing agent, 5-10 parts of chitosan graft modified nanometer SiO2 slurry and 5-10 parts of a flame retardant. With the pouring process, heat energy dissipation in bus operation is facilitated, the expansion coefficient of an epoxy resin in |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN111171515A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN111171515A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN111171515A3</originalsourceid><addsrcrecordid>eNrjZDAOyC8tysxLVygoyk9OLS5WSMsvUihKLc7MU8hNLCnKrFBIzs8tyC_OLElVSCotVkgpTS7hYWBNS8wpTuWF0twMim6uIc4euqkF-fGpxQWJyal5qSXxzn6GQGBuaGpo6mhMjBoAGRoslQ</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Pouring process for resin matrix composite bus duct</title><source>esp@cenet</source><creator>CHEN DINGXUAN ; XIE FEI</creator><creatorcontrib>CHEN DINGXUAN ; XIE FEI</creatorcontrib><description>The invention discloses a pouring process for a resin matrix composite bus duct. The pouring process comprises the following steps of: preparing a mold, and then fixing a busbar in the mold; mixing raw materials of a resin matrix composite according to a ratio at normal temperature, carrying out ultrasonic treatment on the mixed materials under a negative pressure condition, and pumping out escaped foreign gas; conducting pouring under a vacuum condition; and performing curing and demolding at a constant temperature, carrying out trimming and polishing. The resin matrix composite is prepared from the following raw materials in parts by weight: 55-68 parts of epoxy resin, 10-18 parts of acrylic resin, 20-30 parts of glass fibers, 0.5-1 part of aluminum oxide, 2-5 parts of a curing agent, 5-10 parts of chitosan graft modified nanometer SiO2 slurry and 5-10 parts of a flame retardant. With the pouring process, heat energy dissipation in bus operation is facilitated, the expansion coefficient of an epoxy resin in</description><language>chi ; eng</language><subject>CHEMISTRY ; COMPOSITIONS BASED THEREON ; COMPOSITIONS OF MACROMOLECULAR COMPOUNDS ; CONVERSION OR DISTRIBUTION OF ELECTRIC POWER ; ELECTRICITY ; GENERATION ; INSTALLATION OF ELECTRIC CABLES OR LINES, OR OF COMBINEDOPTICAL AND ELECTRIC CABLES OR LINES ; MAKING GRANULES OR PREFORMS ; METALLURGY ; ORGANIC MACROMOLECULAR COMPOUNDS ; PERFORMING OPERATIONS ; PREPARATION OR PRETREATMENT OF THE MATERIAL TO BESHAPED ; RECOVERY OF PLASTICS OR OTHER CONSTITUENTS OF WASTE MATERIALCONTAINING PLASTICS ; THEIR PREPARATION OR CHEMICAL WORKING-UP ; TRANSPORTING ; USE OF INORGANIC OR NON-MACROMOLECULAR ORGANIC SUBSTANCES ASCOMPOUNDING INGREDIENTS ; WORKING OF PLASTICS ; WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL</subject><creationdate>2020</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20200519&DB=EPODOC&CC=CN&NR=111171515A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20200519&DB=EPODOC&CC=CN&NR=111171515A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>CHEN DINGXUAN</creatorcontrib><creatorcontrib>XIE FEI</creatorcontrib><title>Pouring process for resin matrix composite bus duct</title><description>The invention discloses a pouring process for a resin matrix composite bus duct. The pouring process comprises the following steps of: preparing a mold, and then fixing a busbar in the mold; mixing raw materials of a resin matrix composite according to a ratio at normal temperature, carrying out ultrasonic treatment on the mixed materials under a negative pressure condition, and pumping out escaped foreign gas; conducting pouring under a vacuum condition; and performing curing and demolding at a constant temperature, carrying out trimming and polishing. The resin matrix composite is prepared from the following raw materials in parts by weight: 55-68 parts of epoxy resin, 10-18 parts of acrylic resin, 20-30 parts of glass fibers, 0.5-1 part of aluminum oxide, 2-5 parts of a curing agent, 5-10 parts of chitosan graft modified nanometer SiO2 slurry and 5-10 parts of a flame retardant. With the pouring process, heat energy dissipation in bus operation is facilitated, the expansion coefficient of an epoxy resin in</description><subject>CHEMISTRY</subject><subject>COMPOSITIONS BASED THEREON</subject><subject>COMPOSITIONS OF MACROMOLECULAR COMPOUNDS</subject><subject>CONVERSION OR DISTRIBUTION OF ELECTRIC POWER</subject><subject>ELECTRICITY</subject><subject>GENERATION</subject><subject>INSTALLATION OF ELECTRIC CABLES OR LINES, OR OF COMBINEDOPTICAL AND ELECTRIC CABLES OR LINES</subject><subject>MAKING GRANULES OR PREFORMS</subject><subject>METALLURGY</subject><subject>ORGANIC MACROMOLECULAR COMPOUNDS</subject><subject>PERFORMING OPERATIONS</subject><subject>PREPARATION OR PRETREATMENT OF THE MATERIAL TO BESHAPED</subject><subject>RECOVERY OF PLASTICS OR OTHER CONSTITUENTS OF WASTE MATERIALCONTAINING PLASTICS</subject><subject>THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><subject>TRANSPORTING</subject><subject>USE OF INORGANIC OR NON-MACROMOLECULAR ORGANIC SUBSTANCES ASCOMPOUNDING INGREDIENTS</subject><subject>WORKING OF PLASTICS</subject><subject>WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2020</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZDAOyC8tysxLVygoyk9OLS5WSMsvUihKLc7MU8hNLCnKrFBIzs8tyC_OLElVSCotVkgpTS7hYWBNS8wpTuWF0twMim6uIc4euqkF-fGpxQWJyal5qSXxzn6GQGBuaGpo6mhMjBoAGRoslQ</recordid><startdate>20200519</startdate><enddate>20200519</enddate><creator>CHEN DINGXUAN</creator><creator>XIE FEI</creator><scope>EVB</scope></search><sort><creationdate>20200519</creationdate><title>Pouring process for resin matrix composite bus duct</title><author>CHEN DINGXUAN ; XIE FEI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN111171515A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2020</creationdate><topic>CHEMISTRY</topic><topic>COMPOSITIONS BASED THEREON</topic><topic>COMPOSITIONS OF MACROMOLECULAR COMPOUNDS</topic><topic>CONVERSION OR DISTRIBUTION OF ELECTRIC POWER</topic><topic>ELECTRICITY</topic><topic>GENERATION</topic><topic>INSTALLATION OF ELECTRIC CABLES OR LINES, OR OF COMBINEDOPTICAL AND ELECTRIC CABLES OR LINES</topic><topic>MAKING GRANULES OR PREFORMS</topic><topic>METALLURGY</topic><topic>ORGANIC MACROMOLECULAR COMPOUNDS</topic><topic>PERFORMING OPERATIONS</topic><topic>PREPARATION OR PRETREATMENT OF THE MATERIAL TO BESHAPED</topic><topic>RECOVERY OF PLASTICS OR OTHER CONSTITUENTS OF WASTE MATERIALCONTAINING PLASTICS</topic><topic>THEIR PREPARATION OR CHEMICAL WORKING-UP</topic><topic>TRANSPORTING</topic><topic>USE OF INORGANIC OR NON-MACROMOLECULAR ORGANIC SUBSTANCES ASCOMPOUNDING INGREDIENTS</topic><topic>WORKING OF PLASTICS</topic><topic>WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL</topic><toplevel>online_resources</toplevel><creatorcontrib>CHEN DINGXUAN</creatorcontrib><creatorcontrib>XIE FEI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>CHEN DINGXUAN</au><au>XIE FEI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Pouring process for resin matrix composite bus duct</title><date>2020-05-19</date><risdate>2020</risdate><abstract>The invention discloses a pouring process for a resin matrix composite bus duct. The pouring process comprises the following steps of: preparing a mold, and then fixing a busbar in the mold; mixing raw materials of a resin matrix composite according to a ratio at normal temperature, carrying out ultrasonic treatment on the mixed materials under a negative pressure condition, and pumping out escaped foreign gas; conducting pouring under a vacuum condition; and performing curing and demolding at a constant temperature, carrying out trimming and polishing. The resin matrix composite is prepared from the following raw materials in parts by weight: 55-68 parts of epoxy resin, 10-18 parts of acrylic resin, 20-30 parts of glass fibers, 0.5-1 part of aluminum oxide, 2-5 parts of a curing agent, 5-10 parts of chitosan graft modified nanometer SiO2 slurry and 5-10 parts of a flame retardant. With the pouring process, heat energy dissipation in bus operation is facilitated, the expansion coefficient of an epoxy resin in</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | chi ; eng |
recordid | cdi_epo_espacenet_CN111171515A |
source | esp@cenet |
subjects | CHEMISTRY COMPOSITIONS BASED THEREON COMPOSITIONS OF MACROMOLECULAR COMPOUNDS CONVERSION OR DISTRIBUTION OF ELECTRIC POWER ELECTRICITY GENERATION INSTALLATION OF ELECTRIC CABLES OR LINES, OR OF COMBINEDOPTICAL AND ELECTRIC CABLES OR LINES MAKING GRANULES OR PREFORMS METALLURGY ORGANIC MACROMOLECULAR COMPOUNDS PERFORMING OPERATIONS PREPARATION OR PRETREATMENT OF THE MATERIAL TO BESHAPED RECOVERY OF PLASTICS OR OTHER CONSTITUENTS OF WASTE MATERIALCONTAINING PLASTICS THEIR PREPARATION OR CHEMICAL WORKING-UP TRANSPORTING USE OF INORGANIC OR NON-MACROMOLECULAR ORGANIC SUBSTANCES ASCOMPOUNDING INGREDIENTS WORKING OF PLASTICS WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL |
title | Pouring process for resin matrix composite bus duct |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-22T06%3A54%3A03IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=CHEN%20DINGXUAN&rft.date=2020-05-19&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN111171515A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |