Construction method of antibacterial and antifouling building

The invention relates to a construction method of an antibacterial and antifouling building, and belongs to the technical field of antibacterial and antifouling of building construction. The method comprises the following steps: taking 3-4 parts by weight of seashell powder, 5-7 parts by weight of m...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: FU TAO, YAN LUBO, YAN CHENXI, LUAN ZHIMIN, FU GUOXIN, GUO LEI
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The invention relates to a construction method of an antibacterial and antifouling building, and belongs to the technical field of antibacterial and antifouling of building construction. The method comprises the following steps: taking 3-4 parts by weight of seashell powder, 5-7 parts by weight of magnesium oxide and 20-30 parts by weight of paraffin, performing uniform stirring, then adding 10-15parts by weight of side chain amino substituted silicone oil, and performing uniform stirring; and adding 5-7 parts by weight of a coalescing agent before use in order to prepare an antibacterial andantifouling layer. The side chain amino modified silicone oil, the seashell powder, the magnesium oxide and the like are added to improve the binding force with the cement wall surface, the super-hydrophobic property is realized by utilizing the super-strong surface tension, and dusts and the like are not prone to adhering to the cement wall surface. 本发明涉及一种抗菌防污的建筑物的施工方法,属于建筑施工抗菌防污技术领域。取3-4重量份贝壳粉、5-7重量份氧化镁、20-30重量份石蜡,搅拌均匀