Preparation method for new environmentally-friendly anti-corrosion material
The invention provides a preparation method for a new environmentally-friendly anti-corrosion material, and relates to the technical field of filtration. The preparation method comprises the steps that 5-10 parts of polybutadiene resin, 10-15 parts of zinc phosphate, 10-20 parts of micaceous iron ox...
Gespeichert in:
1. Verfasser: | |
---|---|
Format: | Patent |
Sprache: | chi ; eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | The invention provides a preparation method for a new environmentally-friendly anti-corrosion material, and relates to the technical field of filtration. The preparation method comprises the steps that 5-10 parts of polybutadiene resin, 10-15 parts of zinc phosphate, 10-20 parts of micaceous iron oxide, 10-20 parts of crushed crude pearlite and 30-40 parts of butadiene styrene rubber are put intoa stirring device to obtain mixed powder; 10-20 parts of organic silicon resin and 1-5 parts of an anti-settling agent are added into the mixed powder to obtain a liquid mixed raw material; the liquidmixed raw material is transferred into a rubber preparation extrusion device and extruded into a mould, and after primary setting, a green body is formed; the green body obtained after primary setting is flat placed on a flat plate, a mesh structure is pressed on the surface of the green body by using a mesh press mould, and the green body with the mesh structure is vulcanized; environment-friendly coating is sprayed to t |
---|