Method for reducing oil content of oil-containing sludge pyrolyzed product
The invention discloses a method for reducing the oil content of a oil-containing sludge pyrolyzed product. The method comprises the following steps: feeding oil-containing sludge having the oil content of less than 40 percent and water content of less than 70 percent into a high-temperature furnace...
Gespeichert in:
Hauptverfasser: | , , |
---|---|
Format: | Patent |
Sprache: | chi ; eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | The invention discloses a method for reducing the oil content of a oil-containing sludge pyrolyzed product. The method comprises the following steps: feeding oil-containing sludge having the oil content of less than 40 percent and water content of less than 70 percent into a high-temperature furnace; distributing the oil-containing sludge to be 0-80mm thick in the high-temperature furnace; and controlling the pyrolyzing temperature in the high-temperature furnace to be 400-900 DEG C, pyrolyzing for 1-10 hours in an oxygen-free environment to obtain a pyrolyzed product having the oil content reduced to 2 percent or less. According to the method for reducing the oil content of an oil-containing sludge pyrolyzed product, the oil-containing sludge is subjected to oxygen-free pyrolyzing in thehigh-temperature furnace, which is environment-friendly, and the oil content of the oil-containing sludge pyrolyzed product can be well reduced.
本发明公开了种降低含油污泥热解产物含油率的方法,包括以下步骤:将含油率小于40%、含水率小于70%的含油污泥送入高温炉中;所述含油污泥在所述高温炉中的布料厚度为 |
---|