Clean smelting method utilizing nickel-molybdenum ore

The invention relates to a clean smelting method utilizing nickel-molybdenum ore. The clean smelting method comprises the following steps that (1) the nickel-molybdenum ore and pyrolusite are subjected to oxidizing roasting after being mixed evenly to obtain roasted clinkers; and (2) the roasted cli...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: ZHAO TIANYU, LIU XUHENG, ZHAO ZHONGWEI, REN HUICHUAN
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator ZHAO TIANYU
LIU XUHENG
ZHAO ZHONGWEI
REN HUICHUAN
description The invention relates to a clean smelting method utilizing nickel-molybdenum ore. The clean smelting method comprises the following steps that (1) the nickel-molybdenum ore and pyrolusite are subjected to oxidizing roasting after being mixed evenly to obtain roasted clinkers; and (2) the roasted clinkers in the step (1) are added into a phosphoric acid solution for a stirring reaction, and after solid-liquid separation, lixivium including nickel, molybdenum and molybdenum is obtained. By means of the method, the problem of SO2 flue gas pollution existing in the nickel-molybdenum ore smelting process for a long time can be solved, meanwhile, the problem that the reduction cost of low-grade pyrolusite is high can be solved, and a new way is provided for resource utilization of the nickel-molybdenum ore and the pyrolusite. 本发明涉及种镍钼矿的清洁冶炼方法,包括如下步骤:1)将镍钼矿和软锰矿混合均匀后进行氧化焙烧,得到焙烧熟料;2)将步骤1)中所述焙烧熟料加入到磷酸溶液中搅拌反应,固液分离后,得到含镍、锰和钼的浸出液。本发明提出的方法可解决长期以来镍钼矿冶炼过程中SO烟气污染的问题,同时还可解决低品位软锰矿还原成本高的问题,为镍钼矿和软锰矿的资源利用提供新的途径。
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN109280764A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN109280764A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN109280764A3</originalsourceid><addsrcrecordid>eNrjZDB1zklNzFMozk3NKcnMS1fITS3JyE9RKC3JzMmsAgnkZSZnp-bo5ubnVCalpOaV5irkF6XyMLCmJeYUp_JCaW4GRTfXEGcP3dSC_PjU4oLE5NS81JJ4Zz9DA0sjCwNzMxNHY2LUAACOhS2R</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Clean smelting method utilizing nickel-molybdenum ore</title><source>esp@cenet</source><creator>ZHAO TIANYU ; LIU XUHENG ; ZHAO ZHONGWEI ; REN HUICHUAN</creator><creatorcontrib>ZHAO TIANYU ; LIU XUHENG ; ZHAO ZHONGWEI ; REN HUICHUAN</creatorcontrib><description>The invention relates to a clean smelting method utilizing nickel-molybdenum ore. The clean smelting method comprises the following steps that (1) the nickel-molybdenum ore and pyrolusite are subjected to oxidizing roasting after being mixed evenly to obtain roasted clinkers; and (2) the roasted clinkers in the step (1) are added into a phosphoric acid solution for a stirring reaction, and after solid-liquid separation, lixivium including nickel, molybdenum and molybdenum is obtained. By means of the method, the problem of SO2 flue gas pollution existing in the nickel-molybdenum ore smelting process for a long time can be solved, meanwhile, the problem that the reduction cost of low-grade pyrolusite is high can be solved, and a new way is provided for resource utilization of the nickel-molybdenum ore and the pyrolusite. 本发明涉及种镍钼矿的清洁冶炼方法,包括如下步骤:1)将镍钼矿和软锰矿混合均匀后进行氧化焙烧,得到焙烧熟料;2)将步骤1)中所述焙烧熟料加入到磷酸溶液中搅拌反应,固液分离后,得到含镍、锰和钼的浸出液。本发明提出的方法可解决长期以来镍钼矿冶炼过程中SO烟气污染的问题,同时还可解决低品位软锰矿还原成本高的问题,为镍钼矿和软锰矿的资源利用提供新的途径。</description><language>chi ; eng</language><subject>CHEMISTRY ; FERROUS OR NON-FERROUS ALLOYS ; METALLURGY ; PRETREATMENT OF RAW MATERIALS ; PRODUCTION AND REFINING OF METALS ; TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><creationdate>2019</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20190129&amp;DB=EPODOC&amp;CC=CN&amp;NR=109280764A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25562,76317</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20190129&amp;DB=EPODOC&amp;CC=CN&amp;NR=109280764A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>ZHAO TIANYU</creatorcontrib><creatorcontrib>LIU XUHENG</creatorcontrib><creatorcontrib>ZHAO ZHONGWEI</creatorcontrib><creatorcontrib>REN HUICHUAN</creatorcontrib><title>Clean smelting method utilizing nickel-molybdenum ore</title><description>The invention relates to a clean smelting method utilizing nickel-molybdenum ore. The clean smelting method comprises the following steps that (1) the nickel-molybdenum ore and pyrolusite are subjected to oxidizing roasting after being mixed evenly to obtain roasted clinkers; and (2) the roasted clinkers in the step (1) are added into a phosphoric acid solution for a stirring reaction, and after solid-liquid separation, lixivium including nickel, molybdenum and molybdenum is obtained. By means of the method, the problem of SO2 flue gas pollution existing in the nickel-molybdenum ore smelting process for a long time can be solved, meanwhile, the problem that the reduction cost of low-grade pyrolusite is high can be solved, and a new way is provided for resource utilization of the nickel-molybdenum ore and the pyrolusite. 本发明涉及种镍钼矿的清洁冶炼方法,包括如下步骤:1)将镍钼矿和软锰矿混合均匀后进行氧化焙烧,得到焙烧熟料;2)将步骤1)中所述焙烧熟料加入到磷酸溶液中搅拌反应,固液分离后,得到含镍、锰和钼的浸出液。本发明提出的方法可解决长期以来镍钼矿冶炼过程中SO烟气污染的问题,同时还可解决低品位软锰矿还原成本高的问题,为镍钼矿和软锰矿的资源利用提供新的途径。</description><subject>CHEMISTRY</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>METALLURGY</subject><subject>PRETREATMENT OF RAW MATERIALS</subject><subject>PRODUCTION AND REFINING OF METALS</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2019</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZDB1zklNzFMozk3NKcnMS1fITS3JyE9RKC3JzMmsAgnkZSZnp-bo5ubnVCalpOaV5irkF6XyMLCmJeYUp_JCaW4GRTfXEGcP3dSC_PjU4oLE5NS81JJ4Zz9DA0sjCwNzMxNHY2LUAACOhS2R</recordid><startdate>20190129</startdate><enddate>20190129</enddate><creator>ZHAO TIANYU</creator><creator>LIU XUHENG</creator><creator>ZHAO ZHONGWEI</creator><creator>REN HUICHUAN</creator><scope>EVB</scope></search><sort><creationdate>20190129</creationdate><title>Clean smelting method utilizing nickel-molybdenum ore</title><author>ZHAO TIANYU ; LIU XUHENG ; ZHAO ZHONGWEI ; REN HUICHUAN</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN109280764A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2019</creationdate><topic>CHEMISTRY</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>METALLURGY</topic><topic>PRETREATMENT OF RAW MATERIALS</topic><topic>PRODUCTION AND REFINING OF METALS</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>ZHAO TIANYU</creatorcontrib><creatorcontrib>LIU XUHENG</creatorcontrib><creatorcontrib>ZHAO ZHONGWEI</creatorcontrib><creatorcontrib>REN HUICHUAN</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>ZHAO TIANYU</au><au>LIU XUHENG</au><au>ZHAO ZHONGWEI</au><au>REN HUICHUAN</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Clean smelting method utilizing nickel-molybdenum ore</title><date>2019-01-29</date><risdate>2019</risdate><abstract>The invention relates to a clean smelting method utilizing nickel-molybdenum ore. The clean smelting method comprises the following steps that (1) the nickel-molybdenum ore and pyrolusite are subjected to oxidizing roasting after being mixed evenly to obtain roasted clinkers; and (2) the roasted clinkers in the step (1) are added into a phosphoric acid solution for a stirring reaction, and after solid-liquid separation, lixivium including nickel, molybdenum and molybdenum is obtained. By means of the method, the problem of SO2 flue gas pollution existing in the nickel-molybdenum ore smelting process for a long time can be solved, meanwhile, the problem that the reduction cost of low-grade pyrolusite is high can be solved, and a new way is provided for resource utilization of the nickel-molybdenum ore and the pyrolusite. 本发明涉及种镍钼矿的清洁冶炼方法,包括如下步骤:1)将镍钼矿和软锰矿混合均匀后进行氧化焙烧,得到焙烧熟料;2)将步骤1)中所述焙烧熟料加入到磷酸溶液中搅拌反应,固液分离后,得到含镍、锰和钼的浸出液。本发明提出的方法可解决长期以来镍钼矿冶炼过程中SO烟气污染的问题,同时还可解决低品位软锰矿还原成本高的问题,为镍钼矿和软锰矿的资源利用提供新的途径。</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN109280764A
source esp@cenet
subjects CHEMISTRY
FERROUS OR NON-FERROUS ALLOYS
METALLURGY
PRETREATMENT OF RAW MATERIALS
PRODUCTION AND REFINING OF METALS
TREATMENT OF ALLOYS OR NON-FERROUS METALS
title Clean smelting method utilizing nickel-molybdenum ore
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-13T15%3A32%3A59IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=ZHAO%20TIANYU&rft.date=2019-01-29&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN109280764A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true