Method for producing non-oriented electrical steel in endless rolling mode through sheet billets

The invention belongs to the technical field of steel, and particularly relates to a method for producing non-oriented electrical steel in an endless rolling mode through sheet billets. The design components of the non-oriented electrical steel comprise, by mass, 0.0080% or the less of C, 1.0% or th...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: OUYANG YEXIAN, LIANG ZONGREN, CHEN CHAO, YU ZONGJIE, JIN ZHUYUAN, MENG LINGXU, SUN QINGQIANG, ZHENG ZELIN, ZHU JINGTAO, YU YAO, ZHAO RUI, ZHU ZHIQIANG, CHEN CHUANJING, WEN YONGBAO, CHEN LIANG, LIU SHOUJIE, CHEN TONG, ZHENG XUTAO, XU GUANG, XIE JIBIAO
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The invention belongs to the technical field of steel, and particularly relates to a method for producing non-oriented electrical steel in an endless rolling mode through sheet billets. The design components of the non-oriented electrical steel comprise, by mass, 0.0080% or the less of C, 1.0% or the less of Si, 0.010% or the less of Als, 0.5% or the less of Mn, 0.05% or the less of P, 0.008% or the less of S, 0.0080% or the less of N and the balance Fe and inevitable impurities. 本申请属于于钢铁技术领域,具体为种采用薄板坯无头轧制生产无取向电工钢的方法。无取向电工钢成分设计的质量百分比为:C≤0.0080%,Si≤1.0%,Als≤0.010%,Mn≤0.5%,P≤0.05%,S≤0.008%,N≤0.0080%,其余为铁和不可避免的杂质。