Method for plasma nitriding at room temperature to prepare nanocrystal titanium nitride micropowder

The invention belongs to the technical field of metal nitride, and discloses a method of plasma nitriding at the room temperature to prepare nanocrystal titanium nitride micropowder. The method comprises the steps that under an atmosphere that nitrogen is continuously supplied, a plasma ball milling...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: LU ZHONGCHEN, BAO XIANYONG, OUYANG LIUZHANG, ZHANG FENG, ZENG MEIQIN, CHEN ZUJIAN, ZHU MIN, JIN LEI
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator LU ZHONGCHEN
BAO XIANYONG
OUYANG LIUZHANG
ZHANG FENG
ZENG MEIQIN
CHEN ZUJIAN
ZHU MIN
JIN LEI
description The invention belongs to the technical field of metal nitride, and discloses a method of plasma nitriding at the room temperature to prepare nanocrystal titanium nitride micropowder. The method comprises the steps that under an atmosphere that nitrogen is continuously supplied, a plasma ball milling device is adopted to conduct plasma nitriding ball milling on titanium powder at the room temperature, and the nanocrystal titanium nitride micropowder is obtained. The plasma is dielectric barrier discharging plasma. The specific parameters of plasma nitriding ball milling at the room temperatureare: the rotation speed is 600-1200rpm, the discharging current is 1-2.5A, the ratio of grinding media to material is 30:1-100:1, the ball milling time is 10-30 hours, and the pressure intensity of nitrogen is 0.05MPa-0.5MPa. The method is easy to operate and low in cost, the atmosphere pressure intensity is controllable and adjustable, the ball milling pollution is less, the grain size of the synthesized titanium nitride
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN108752006A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN108752006A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN108752006A3</originalsourceid><addsrcrecordid>eNqNizsKAjEQQLexEPUO4wGEqPhpZVFstLJfhmRWA0lmmMwi3l6LPYDVe8V708bfyF4coGcFSVgzQommMcTyBDRQ5gxGWUjRBiUwBlES_GnBwl4_1TCBRcMShzzeBDl6ZeF3IJ03kx5TpcXIWbO8nB_tdUXCHVVBT4Wsa-9rdzzsNs7tT9t_mi8Mkz93</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Method for plasma nitriding at room temperature to prepare nanocrystal titanium nitride micropowder</title><source>esp@cenet</source><creator>LU ZHONGCHEN ; BAO XIANYONG ; OUYANG LIUZHANG ; ZHANG FENG ; ZENG MEIQIN ; CHEN ZUJIAN ; ZHU MIN ; JIN LEI</creator><creatorcontrib>LU ZHONGCHEN ; BAO XIANYONG ; OUYANG LIUZHANG ; ZHANG FENG ; ZENG MEIQIN ; CHEN ZUJIAN ; ZHU MIN ; JIN LEI</creatorcontrib><description>The invention belongs to the technical field of metal nitride, and discloses a method of plasma nitriding at the room temperature to prepare nanocrystal titanium nitride micropowder. The method comprises the steps that under an atmosphere that nitrogen is continuously supplied, a plasma ball milling device is adopted to conduct plasma nitriding ball milling on titanium powder at the room temperature, and the nanocrystal titanium nitride micropowder is obtained. The plasma is dielectric barrier discharging plasma. The specific parameters of plasma nitriding ball milling at the room temperatureare: the rotation speed is 600-1200rpm, the discharging current is 1-2.5A, the ratio of grinding media to material is 30:1-100:1, the ball milling time is 10-30 hours, and the pressure intensity of nitrogen is 0.05MPa-0.5MPa. The method is easy to operate and low in cost, the atmosphere pressure intensity is controllable and adjustable, the ball milling pollution is less, the grain size of the synthesized titanium nitride</description><language>chi ; eng</language><subject>ARTIFICIAL STONE ; CEMENTS ; CERAMICS ; CHEMISTRY ; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS ; CONCRETE ; LIME, MAGNESIA ; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES ; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES ; METALLURGY ; NANOTECHNOLOGY ; PERFORMING OPERATIONS ; REFRACTORIES ; SLAG ; SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES ; TRANSPORTING ; TREATMENT OF NATURAL STONE</subject><creationdate>2018</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20181106&amp;DB=EPODOC&amp;CC=CN&amp;NR=108752006A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20181106&amp;DB=EPODOC&amp;CC=CN&amp;NR=108752006A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>LU ZHONGCHEN</creatorcontrib><creatorcontrib>BAO XIANYONG</creatorcontrib><creatorcontrib>OUYANG LIUZHANG</creatorcontrib><creatorcontrib>ZHANG FENG</creatorcontrib><creatorcontrib>ZENG MEIQIN</creatorcontrib><creatorcontrib>CHEN ZUJIAN</creatorcontrib><creatorcontrib>ZHU MIN</creatorcontrib><creatorcontrib>JIN LEI</creatorcontrib><title>Method for plasma nitriding at room temperature to prepare nanocrystal titanium nitride micropowder</title><description>The invention belongs to the technical field of metal nitride, and discloses a method of plasma nitriding at the room temperature to prepare nanocrystal titanium nitride micropowder. The method comprises the steps that under an atmosphere that nitrogen is continuously supplied, a plasma ball milling device is adopted to conduct plasma nitriding ball milling on titanium powder at the room temperature, and the nanocrystal titanium nitride micropowder is obtained. The plasma is dielectric barrier discharging plasma. The specific parameters of plasma nitriding ball milling at the room temperatureare: the rotation speed is 600-1200rpm, the discharging current is 1-2.5A, the ratio of grinding media to material is 30:1-100:1, the ball milling time is 10-30 hours, and the pressure intensity of nitrogen is 0.05MPa-0.5MPa. The method is easy to operate and low in cost, the atmosphere pressure intensity is controllable and adjustable, the ball milling pollution is less, the grain size of the synthesized titanium nitride</description><subject>ARTIFICIAL STONE</subject><subject>CEMENTS</subject><subject>CERAMICS</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</subject><subject>CONCRETE</subject><subject>LIME, MAGNESIA</subject><subject>MANUFACTURE OR TREATMENT OF NANOSTRUCTURES</subject><subject>MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES</subject><subject>METALLURGY</subject><subject>NANOTECHNOLOGY</subject><subject>PERFORMING OPERATIONS</subject><subject>REFRACTORIES</subject><subject>SLAG</subject><subject>SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES</subject><subject>TRANSPORTING</subject><subject>TREATMENT OF NATURAL STONE</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2018</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNizsKAjEQQLexEPUO4wGEqPhpZVFstLJfhmRWA0lmmMwi3l6LPYDVe8V708bfyF4coGcFSVgzQommMcTyBDRQ5gxGWUjRBiUwBlES_GnBwl4_1TCBRcMShzzeBDl6ZeF3IJ03kx5TpcXIWbO8nB_tdUXCHVVBT4Wsa-9rdzzsNs7tT9t_mi8Mkz93</recordid><startdate>20181106</startdate><enddate>20181106</enddate><creator>LU ZHONGCHEN</creator><creator>BAO XIANYONG</creator><creator>OUYANG LIUZHANG</creator><creator>ZHANG FENG</creator><creator>ZENG MEIQIN</creator><creator>CHEN ZUJIAN</creator><creator>ZHU MIN</creator><creator>JIN LEI</creator><scope>EVB</scope></search><sort><creationdate>20181106</creationdate><title>Method for plasma nitriding at room temperature to prepare nanocrystal titanium nitride micropowder</title><author>LU ZHONGCHEN ; BAO XIANYONG ; OUYANG LIUZHANG ; ZHANG FENG ; ZENG MEIQIN ; CHEN ZUJIAN ; ZHU MIN ; JIN LEI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN108752006A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2018</creationdate><topic>ARTIFICIAL STONE</topic><topic>CEMENTS</topic><topic>CERAMICS</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</topic><topic>CONCRETE</topic><topic>LIME, MAGNESIA</topic><topic>MANUFACTURE OR TREATMENT OF NANOSTRUCTURES</topic><topic>MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES</topic><topic>METALLURGY</topic><topic>NANOTECHNOLOGY</topic><topic>PERFORMING OPERATIONS</topic><topic>REFRACTORIES</topic><topic>SLAG</topic><topic>SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES</topic><topic>TRANSPORTING</topic><topic>TREATMENT OF NATURAL STONE</topic><toplevel>online_resources</toplevel><creatorcontrib>LU ZHONGCHEN</creatorcontrib><creatorcontrib>BAO XIANYONG</creatorcontrib><creatorcontrib>OUYANG LIUZHANG</creatorcontrib><creatorcontrib>ZHANG FENG</creatorcontrib><creatorcontrib>ZENG MEIQIN</creatorcontrib><creatorcontrib>CHEN ZUJIAN</creatorcontrib><creatorcontrib>ZHU MIN</creatorcontrib><creatorcontrib>JIN LEI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>LU ZHONGCHEN</au><au>BAO XIANYONG</au><au>OUYANG LIUZHANG</au><au>ZHANG FENG</au><au>ZENG MEIQIN</au><au>CHEN ZUJIAN</au><au>ZHU MIN</au><au>JIN LEI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Method for plasma nitriding at room temperature to prepare nanocrystal titanium nitride micropowder</title><date>2018-11-06</date><risdate>2018</risdate><abstract>The invention belongs to the technical field of metal nitride, and discloses a method of plasma nitriding at the room temperature to prepare nanocrystal titanium nitride micropowder. The method comprises the steps that under an atmosphere that nitrogen is continuously supplied, a plasma ball milling device is adopted to conduct plasma nitriding ball milling on titanium powder at the room temperature, and the nanocrystal titanium nitride micropowder is obtained. The plasma is dielectric barrier discharging plasma. The specific parameters of plasma nitriding ball milling at the room temperatureare: the rotation speed is 600-1200rpm, the discharging current is 1-2.5A, the ratio of grinding media to material is 30:1-100:1, the ball milling time is 10-30 hours, and the pressure intensity of nitrogen is 0.05MPa-0.5MPa. The method is easy to operate and low in cost, the atmosphere pressure intensity is controllable and adjustable, the ball milling pollution is less, the grain size of the synthesized titanium nitride</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN108752006A
source esp@cenet
subjects ARTIFICIAL STONE
CEMENTS
CERAMICS
CHEMISTRY
COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS
CONCRETE
LIME, MAGNESIA
MANUFACTURE OR TREATMENT OF NANOSTRUCTURES
MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES
METALLURGY
NANOTECHNOLOGY
PERFORMING OPERATIONS
REFRACTORIES
SLAG
SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES
TRANSPORTING
TREATMENT OF NATURAL STONE
title Method for plasma nitriding at room temperature to prepare nanocrystal titanium nitride micropowder
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-04T20%3A21%3A47IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=LU%20ZHONGCHEN&rft.date=2018-11-06&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN108752006A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true