Mullite crystal whisker doped corundum-mullite load bearing board and preparation method thereof
The invention relates to a mullite crystal whisker doped corundum-mullite load bearing board. The mullite crystal whisker doped corundum-mullite load bearing board comprises the following raw materials in parts by mass: 35-55 parts of corundum, 20-30 parts of mullite, 20-40 parts of aluminum oxide m...
Gespeichert in:
Hauptverfasser: | , , , , , , , , |
---|---|
Format: | Patent |
Sprache: | chi ; eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | The invention relates to a mullite crystal whisker doped corundum-mullite load bearing board. The mullite crystal whisker doped corundum-mullite load bearing board comprises the following raw materials in parts by mass: 35-55 parts of corundum, 20-30 parts of mullite, 20-40 parts of aluminum oxide micro powder, 5-15 parts of kaolin, and 1-5 parts of mullite crystal whiskers. The invention also provides a preparation method of the mullite crystal whisker doped corundum-mullite load bearing board. The mullite crystal whisker doped corundum-mullite load bearing board provided by the invention hasthe advantages of good thermal shock resistance, high-temperature resistance, high strength, high hardness and corrosion resistance, and has a good use effect, long service life and simple preparation.
本发明涉及种莫来石晶须掺杂刚玉-莫来石承烧板,所述莫来石晶须掺杂刚玉-莫来石承烧板包括以下质量份数的原料:刚玉35~55份、莫来石20~30份、氧化铝微粉20~40份、高岭土5~15份、莫来石晶须1~5份。本发明还提供种莫来石晶须掺杂刚玉-莫来石承烧板的制造方法。本发明的莫来石晶须掺杂刚玉-莫来石承烧板具有抗热震性好、耐高温、强度高、硬度大、耐腐蚀的优点,且使用效果好,使用寿命长,制备简单。 |
---|